D5327 Standard Practice for Evaluating and Comparing Transfer Efficiency of Spray Applied Coatings Under General Laboratory Conditions

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: August 21, 2007
Editorial Change:
 
1.1 This practice covers the evaluation and comparison of the transfer efficiency of spray-applied coatings under general laboratory conditions. Transfer efficiency is the ratio of paint solids deposited to the total paint solids used during the application process, expressed as a percent. This practice can be used to study the effect on transfer efficiency of changing operating variables and paint formulations. Key variables that need to be controlled are listed in 8.13.

Note 1 - It is important that all process or formulation parameters, except that which is intentionally being changed, be kept consistent from test to test. If not done, the results of the study are to be questioned.

1.2 The reproducibility of this practice is highly dependent on the degree of control of the parameters listed in Section 8 of the practice.

1.3 Limitations - This laboratory practice indicates only the direction of the effect of operating variables and liquid paint formulations on transfer efficiency under conditions of the laboratory test: the magnitude of the effect can be determined only with specific plant experience. In fact, the nature of the critical parameters that affect transfer efficiency makes clear that it is not possible to extrapolate laboratory results.

Note 2 - The laboratory practice outlined involves general laboratory spray equipment and procedures and is derived from Test Method D 5009. This practice and Test Method D 5009 are both derived from a study and report of transfer efficiency measurements conducted for the U.S. Environmental Protection Agency. For laboratories that have access to a conveyor and mass flow measurement equipment, a suitable, potentially more reproducible, tested method is defined in Test Method D 5009.

1.4 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

(Back to all Standards)

 
   

Abrasives Inc.
See the difference immediately Black Magic®

Quality blast abrasive goes farther. Use Black Magic® The Tough Stuff coal slag. Cleaner, consistent, less dust. Order yours today!
Abrasives Inc. 800-584-7524


HoldTight Solutions Inc.
NO FLASH RUST -
NO CONTAMINANTS

Our HoldTight®102 salt remover & flash rush inhibitor prevents flash rust by removing surface contaminants.
Contact us for your nearest distributor. (800) 319.8802 sales@holdtight.com


NLB Corporation
Handheld VertaJet™ for concrete or steel

Ergonomic VertaJet from NLB boosts surface prep productivity. Rotating 40,000 psi water jets strip a 6” path and get into corners, with vacuum recovery.


No Ordinary Soda
ARMEX® baking soda-based abrasives from the makers of ARM & HAMMER® products offers over 12 formulas specially engineered for your application and your budget.


Mascoat
Global Leader In Thermal Insulating Coatings

Our coatings are uniquely engineered and manufactured in-house to fulfill market-specific needs, enhance energy retention, prevent CUI and protect personnel.


Absolute Equipment/Grand Rental Station
Portable Power from Absolute Equipment

•Compressors
•Lighting Systems
•Generators
•Light Compaction
Sales • Rental • Service
Call 1-866-931-6655
Over a century of
providing excellence.


Corrosion Probe, Inc.
From Detection to Correction

Corrosion Probe, Inc. has the Most Concrete Coatings Experience and Expertise. Contact us today at
860-767-4402, www.cpiengineering.com

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com