D268 Standard Guide for Sampling and Testing Volatile Solvents and Chemical Intermediates for Use in Paint and Related Coatings and Material

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: September 20, 2012
Updated On: October 01, 2012
Editorial Change:
 
1.1 This guide covers procedures for the sampling and testing of volatile solvents used in the manufacture of paint, lacquer, varnish, and related products. The test methods are listed in Table 1.

1.2 For specific hazard information and guidance, see Suppliers' Material Safety Data Sheet for materials listed in this guide.

1.3 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

This standard does not purport to address the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to consult and establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   

Greenhorne & O'Mara, Inc.
One Team. Infinite Solutions.

Greenhorne & O’Mara is now Stantec. Contact us for coatings and corrosion consulting, design, analysis, and inspection services at john.woods@stantec.com.


PreTox Products - NexTec, Inc.
GOT LEAD? Specify Pretox System products

The ONLY Lead Stabilizer Compatible with All Paint Removal Methods. Works with all Blast Media: Grits | Recyclable Abrasives | CO2 | Water | Power Tools | Etc. Call Dave Steffen at 800.338.8296.


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Truss bridge treated in 2000 with Termarust's (HR CSA) field-proven rust mitigation system chemically stopped corrosion, crevice corrosion & pack rust.


GMA Garnet USA
GMA Garnet™
Natural Abrasives

- Superior cleaning performance
- Even Profile
- Low Dust
- Cost-Effective
- Environmentally friendly
- Recyclable up to 5 times
Tel : +1 832 243 9300


DeLong Equipment
Delong Equipment Co.
Blast Equipment Products

"The Delong Equipment Company .….supplying abrasive blast equipment, parts and abrasives to blasting contractors, manufacturers and industry for over 45 years”


Van Air Systems
The Blast Pak

Van Air Systems' portable desiccant air dryer. Get dry compressed air with this All-In-One blasting and coating solution.


Madison Chemical Industries Inc.
Coat steel without blasting

Madison’s No-Blast technology
eliminates the need for
abrasive blasting in a number
of service applications.
See it in action at
MadisonChemical.com.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com