C1315 Standard Specification for Liquid Membrane-Forming Compounds Having Special Properties for Curing and Sealing Concrete

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: June 27, 2011
Updated On: June 28, 2011
Editorial Change:
 
This specification covers the performance requirements for membrane-forming liquids suitable for use as curing compounds and sealers for fresh and hardened concrete. Each membrane should have good alkali resistance, acid resistance, adhesion-promoting qualities, and resistance to degradation by UV light. The materials are limited to clear or translucent and white pigmented materials, all of which are classified into non-yellowing, moderately yellowing, or yellows or darkens unrestrictedly.

(Back to all Standards)

 
   

DRYCO
The one way to control
a tank: DRYCO

Temporary climate control equipment. Dehumidifiers,
Heaters, A/C, Power, More…
Toll Free: 866-379-2600


NLB Corporation
Handheld VertaJet™ for concrete or steel

Ergonomic VertaJet from NLB boosts surface prep productivity. Rotating 40,000 psi water jets strip a 6” path and get into corners, with vacuum recovery.


Safway Services
Suspended Access Made Easy With QuikDeck™

The smart choice for suspended access, QuikDeck’s interchangeable, lightweight components make them easy to set up and reassemble when you need to move.


SAFE Systems, Inc.
Portable Dust Collectors for Tough Environments

Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.


Rapid Prep, LLC
Nation Wide Equipment Rentals

Rapid Prep, LLC is a full service provider of sandblasting & all other surface preparation equipment, with 60 years of experience within the industrial painting industry.


Corrosion Specialties, Inc.
The T93R Airless
Tip System

is the longest lasting, highest quality tip and guard available to coatings applicators around the world. Click the link to contact Corrosion Specialties.


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Hydro Utility Penstock Overcoated in 1997. Was power washed and overcoated with major cost saving. No environmental impact with Termarust's low LC50 of 41,007 ppm.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com