C1017 Standard Specification for Chemical Admixtures for Use in Producing Flowing Concrete

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 24, 2007
Editorial Change:
 
1.1 This specification covers two types of chemical admixtures to be added to hydraulic cement concrete mixtures for the purpose of producing flowing concrete. The types are as follows: 1.1.1 Type I - Plasticizing, and 1.1.2 Type II - Plasticizing and retarding.

1.2 This specification stipulates tests of a chemical admixture with reference concreting materials or with concrete-making materials proposed for specific work. Unless otherwise specified by the purchaser, the tests shall be made using reference concreting materials.

1.3 If a chemical admixture has been tested and found to comply with the provisions of this specification using reference materials, and is being considered for use with other materials for specific work, additional tests for such use are allowed if agreed upon between the purchaser and the supplier and are allowed to consist of a portion of the tests described herein.

1.4 This specification provides for three levels of testing. 1.4.1 Level 1 - During the initial approval stage, proof of compliance with the performance requirements defined in demonstrates that the admixture meets the requirements of this specification. Uniformity and equivalence tests of the section on Lot Uniformity and Equivalence shall be carried out to provide results against which later comparisons can be made.

1.4.2 Level 2 - Limited retesting described in the section relating to general requirements may be requested at intervals by the purchaser. Proof of compliance with the requirements of demonstrates continued conformity of the admixture with the requirements of the specification.

1.4.3 Level 3 - For acceptance of a lot or for measuring uniformity within or between lots, when specified by the purchaser, the uniformity and equivalence tests of the section on Lot Uniformity and Equivalence shall be used.

(Back to all Standards)

 
   
Advertisements
 
KTA-Tator, Inc. - Corporate Office
 
Instrument Service Department
 
Are you a QP certified contractor? KTA’s Instrument Service Department can help keep you compliant!
Click or call 1-800-KTA-GAGE.
 

 
Fischer Technology Inc.
 
FISCHER Expands Corrosion Product Line
 
Rounding out Fischer’s extensive line of products for measuring protective coatings in the corrosion industry is the new ultrasonic wall thickness gauge UMP series.
 

 
SAFE Systems, Inc.
 
Custom blast rooms
by SAFE Systems
 
Don't waste time and money "making do" with a "standard" design. Let us work with you to design and build the system that best fits your requirements.
Call 1-800-634-7278
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
ARC / A.W. Chesterton Company
 
Superior Impact & Wear Resistant Lining
 
100% solids, impact resistant, ceramic reinforced, epoxy/urethane hybrid lining for severe abrasive wear and impact resistance.
 

 
SABRE Autonomous Solutions
 
Introducing the ALPHA1 Blasting Robot
 
Once installed and commissioned – simply
SCAN PLAN BLAST.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us