D907 Standard Terminology of Adhesives

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: September 24, 2012
Updated On: October 01, 2012
Editorial Change:
 
1.1 This terminology standard is a compilation of definitions used in the science and technology of the adhesives industry. Terms that are generally understood or adequately defined in other readily available sources are not included.

1.2 Any changes in this standard since 1988 are documented as follows: 1.2.1 gives a history of revisions made since 1988. lists the terms that are affected as: (1) Terms Added, (2) Terms Revised, and (3) Terms Deleted.

In , the year of publication in Volume 15.06 is shown in parentheses following the term.

1.2.2 In the text of the standard, the year of publication is shown following each definition. Also, the following codes are included after the year of publication to describe the type change that was made: (A) Addition, (R) Revision, or (E) Edited.

1.2.3 Deletions are shown in , suitably footnoted. The deleted terms do not appear in the text of the standard.

1.2.4 Any special circumstances not covered by and are documented in , suitably footnoted.

(Back to all Standards)

 
   

Abrasives Inc.
See the difference immediately Black Magic®

Quality blast abrasive goes farther. Use Black Magic® The Tough Stuff coal slag. Cleaner, consistent, less dust. Order yours today!
Abrasives Inc. 800-584-7524


Madison Chemical Industries Inc.
There’s only one CorroCote

Madison invented CorroCote
in 1974 to prevent corrosion
in underground fuel storage
tanks. Today, it’s still the
classic coating for protecting
infrastructure


Absolute Equipment/Grand Rental Station
Portable Power from Absolute Equipment

•Compressors
•Lighting Systems
•Generators
•Light Compaction
Sales • Rental • Service
Call 1-866-931-6655
Over a century of
providing excellence.


SAFE Systems, Inc.
Enduroguard -
The Tough Cable
for a Tough Industry.

Reduce maintenance costs and down time, increase job site safety with Enduroguard Cable. Available exclusively from SAFE Systems. UL listed, flexible, abrasion resistant and cut resistant.


International Paint LLC
Our New Protective Coatings Centers

Our complete range of International and Devoe Coatings products are available at our Protective Coatings Centers, making purchases faster and easier.


DRYCO
The one way to control
a tank: DRYCO

Temporary climate control equipment. Dehumidifiers,
Heaters, A/C, Power, More…
Toll Free: 866-379-2600


ITW Binks
Built for Tough Jobs

From Epoxies to Urethanes to other high solid coatings, the new Binks Airless 75 delivers a great finish using an ergonomic design. Visit binks.com for more information.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com