SP0592-2006 Application of a Coating System to Interior Surfaces of New and Used Rail Tank Cars in Concentrated (90 to 98%) Sulfuric Acid Service

All Standards | NACE Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 23, 2012
Editorial Change:
 
Reaffirmed in 2006. Addresses the need for high-quality application of coatings to the interior surfaces of rail tank cars handling shipments of concentrated sulfuric acid at ambient temperatures. Qualified inspection of the completed coating system and testing by the use of adequate, readily available instruments are also covered. Sections include information on areas of responsibility, surface preparation, coating system materials and application, coating of particular parts and attachments, and inspection. A tank car coating system inspection report form and a listing of essential facilities and equipment for application of a coating system to the interior of tank cars for concentrated sulfuric acid service are also included. Keywords: protective coatings, rail cars, sulfuric acid handling, tanks.

(Back to all Standards)

 
   

3M Corrosion Protection Products
3M™ Sotchkote™ 323 Field Applied Coatings

Let 3M show you how 50 years of experience can lead to less waste, less rework, and more productivity. Our coatings are proudly made in the U.S.A. go.3M.com/Find/Distributor


Atlantic Design, Inc.
We’ve Got a Surprise For You!

We’ve designed two new lines
of equipment with shorter lead
times, budget friendly prices,
more safety features & all
with the same ADI quality!
866.Call.ADI


Denso North America Inc.
Tank Base Protection

An easy to apply system utilizing Denso tapes and coatings around the tank base, that helps prevent corrosion from external elements.
Call 1-281-821-3355 or Visit densona.com


EnTech Industries, Inc.
EnTech Dust Collectors in Stock & Ready to Ship

2,000 cfm to 80,000 cfm Units
Diesel * Electric * Bi-Powered
* Mobile Trailer Mounted
* Custom Designs and Colors
Find a Dealer near You
Call 1-800-733-5384


International Paint LLC
Our New Protective Coatings Centers

Our complete range of International and Devoe Coatings products are available at our Protective Coatings Centers, making purchases faster and easier.


HoldTight Solutions Inc.
NO FLASH RUST -
NO CONTAMINANTS

Our HoldTight®102 salt remover & flash rush inhibitor prevents flash rust by removing surface contaminants.
Contact us for your nearest distributor. (800) 319.8802 sales@holdtight.com


Blastox/The TDJ Group, Inc.
Blastox - One Step
Lead Abatement

Don't waste $$ on added labor steps with other methods. Don't mix, meter or apply at the job-site. Avoid strict hazardous waste rules.
Let your painters paint!

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com