D7127 D7127-05 Standard Test Method for Measurement of Surface Roughness of Abrasive Blast Cleaned Metal Surfaces Using a Portable Stylus Instrument

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: January 25, 2006
Editorial Change:
 
1.1 This test method describes a shop or field procedure for determination of four roughness characteristics of surfaces prepared for painting by abrasive blasting. The procedure uses a portable skidded or non-skidded stylus profile tracing instrument. The three measured characteristics are: Rt, Rmax, and Pc.

1.2 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

1.3 In general, this method should be limited to the measurement of surface roughness where Rmax is in the range 10 to 150 m (0.4 to 6 mil) and where the Peak Count, Pc, is less than 180 peaks/cm (450 peaks/in.).

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   

Bayer MaterialScience LLC
Desmodur® XP 2763 Drives Financial Results

High performance polyaspartic coatings
• Dry faster
• Fewer coats
• Superior corrosion/weather resistance
412-777-3983


TruQC, LLC
Click here to start your free trial

TruQC is cloud-based job-site documentation built for the iPad. It's easy-to-use, objective and complies to common industry standards. Learn more: TruQCApp.com.


Axxiom Manufacturing
Schmidt Improves
Portable Blasters

Schmidt's VBS System reduces blowdown intensity, prevents exhaust from damaging floor while using no screens or filters. Reduces sound; Increasing safety.
Call 1-800-231-2085


Dow Corning Corporation
New Dow Corning® 3055 Resin

Ensure long-term asset protection and extend repaint cycles with a low-VOC, two-coat polysiloxane coating featuring superior corrosion and moisture resistance.


Atlantic Design, Inc.
We’ve Got a Surprise For You!

We’ve designed two new lines
of equipment with shorter lead
times, budget friendly prices,
more safety features & all
with the same ADI quality!
866.Call.ADI


Corrocoat USA Inc.
Corrosion Solutions for Aggressive Environments

Engineering thick film polymer linings for tanks, vessels, valves, pumps, pipes and concrete since 1975.


US Minerals
US Minerals -
Black Magnum

With nationwide production and distribution capabilities, U.S. Minerals supplies a complete range of coal slag and other abrasives to meet all of your blasting needs.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com