C303-02 Concrete Pressure Pipe, Bar-Wrapped, Steel-Cylinder Type

All Standards | AWWA Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 25, 2012
Editorial Change:
 
This standard covers the manufacture of concrete pressure pipe, reinforced with a steel cylinder that is helically wrapped with mild steel bar reinforcement, in sizes ranging from 10 in. through 60 in. (250 mm through 1,520 mm), inclusive, and for working pressures up to 400 psi (2,760 kPa). Larger pipe sizes and pipe accommodating higher pressures have been manufactured based on the concepts of this standard. With agreement by the purchaser and the manufacturer, pipe may be manufactured to larger sizes and for higher pressures than indicated herein. This standard does not include requirements for design, handling, delivering, laying, field testing, or disinfecting of pipe and fittings. The pipe shall have the following principal features: a welded steel cylinder with sized steel joint rings welded to the ends; a lining of concrete or cement mortar centrifugally applied within the steel cylinder and spigot ring; reinforcement consisting of continuous steel bar helically wound tightly around the outside of the cylinder and securely fastened by welding to the steel joint ring at each end of the cylinder; a coating of dense mortar covering the cylinder and bars, except for the necessarily exposed surfaces of the spigot joint ring; and a self-centering joint with a preformed gasket of rubber, so designed that the joint will be watertight under all conditions of service.

(Back to all Standards)

 
   

Modern Safety Techniques
Modern Safety Techniques

With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern


Safety Lamp of Houston, Inc.
Wet & hazardous area lighting solutions from SAFETY LAMP of Houston

New WOLF LED and fluorescent lights are now available, including low voltage tank lighting kits.
Call: (281) 964-1019.


Dampney Co., Inc.
Solar Coating

High Temperature Resistant for Solar Panels/Collectors/Tubes. Achieve selectivity with the economy and ease
of application of a paint.


DeHumidification Technologies
HUMIDITY PROBLEMS?

DH Tech has the most innovative and reliable equipment available to
control humidity efficiently
and effectively.
IT'S UNDER CONTROL!


DRYCO
Environmental Controls
Equipment & Service

Temporary climate control equipment. Dehumidifiers,
Heaters, A/C, Power, More…
Toll Free: 866-379-2600


Abrasives Inc.
See the difference immediately Black Magic®

Quality blast abrasive goes farther. Use Black Magic® The Tough Stuff coal slag. Cleaner, consistent, less dust. Order yours today!
Abrasives Inc. 800-584-7524


TruQC, LLC
Click here to start your free trial

TruQC is cloud-based job-site documentation built for the iPad. It's easy-to-use, objective and complies to common industry standards. Learn more: TruQCApp.com.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com