A849 Standard Specification for Post-Applied Coatings, Pavings, and Linings for Corrugated Steel Sewer and Drainage Pipe

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: December 13, 2005
Editorial Change:
 
1.1 This specification covers post-applied coatings, pavings, and linings for corrugated steel pipe and corrugated steel structural plate pipe, pipe-arches, and arches coated, paved, or lined with specified materials over either metallic coatings or metallic coatings with polymer coatings. This specification includes asphalt, polymerized asphalt, polymer, mastic, and emulsion coatings and asphalt and concrete pavements and linings applied to the pipe in the producing plant, as well as, asphalt and mastic coatings applied in the field. Field-applied concrete pavements and linings are covered by Specification A979/A979M. The pipe to which the coatings are applied is described in Specifications A760/A760M, A761/A761M, and A762/ A762M.

1.2 There is no cleaning operation currently included in pipe coating practice. However, experience has shown that a clean substrate provides good adherence for both cold- and hot-applied post coatings. The performance of post coating or lining, or both, will depend on the surface cleanliness over which it is applied.

1.3 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are for information only.

1.4 The following safety hazards caveat pertains only to the test methods portions, Sections 10 and 11, of this specification. This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   

Greenhorne & O'Mara, Inc.
One Team. Infinite Solutions.

Greenhorne & O’Mara is now Stantec. Contact us for coatings and corrosion consulting, design, analysis, and inspection services at john.woods@stantec.com.


Corrocoat USA Inc.
Corrosion Solutions for Aggressive Environments

Engineering thick film polymer linings for tanks, vessels, valves, pumps, pipes and concrete since 1975.


HoldTight Solutions Inc.
NO FLASH RUST -
NO CONTAMINANTS

Our HoldTight®102 salt remover & flash rush inhibitor prevents flash rust by removing surface contaminants.
Contact us for your nearest distributor. (800) 319.8802 sales@holdtight.com


Fox Industries Inc.
Repair, Protect & Strengthen

Need a coating? Turn to Fox. We have solutions to repair, protect and strengthen concrete, steel and wood substrates. Call 888-760-0369 or email info@foxind.com


Clemco Industries Corp.
Powerful Protection in a Small Package

Mounts inside blast helmet, alerts operator to dangerous breathing-air condition by audible, visual, and vibratory alarms. Easily calibrated, battery operated.


EDCO - Equipment Development Co. Inc.
EDCO's Quick Response Codes

EDCO now includes Quick Response Code decals on machines. These QRC's provide customers with instant jobsite advice, problem solving tips and much more. Click to watch EDCO machines in action.


Versaflex Inc.
Best NSF 61.5 Approved Potable Water Polyurea

VersaFlex Polyurea Earns Highest ANSI/NSF 61.5 Rating for High Temp Service, Minimum Tank Size and Max Thickness. All Polyureas Are Not Created Equal. FREE WHITE PAPER.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com