C618 Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: March 26, 2012
Updated On: April 04, 2012
Editorial Change:
 
This specification covers coal fly ash and raw or calcined natural pozzolan for use in concrete where cementitious or pozzolanic action, or both, is desired, or where other properties normally attributed to fly ash or pozzolans may be desired, or where both objectives are to be achieved. Fly ash and natural pozzolans shall conform to the prescribed chemical composition requirements and physical requirements. The materials shall be tested for fineness, strength activity index, water requirement, soundness, and autoclave expansion or contraction.

(Back to all Standards)

 
   

Empire Scaffold
Work with a scaffold company you can trust

Empire Scaffold is a full-service scaffold company providing specialized, on-site support for the life of the project, with products & experience to keep your projects up & running, safely.


Absolute Equipment/Grand Rental Station
Portable Power from Absolute Equipment

•Compressors
•Lighting Systems
•Generators
•Light Compaction
Sales • Rental • Service
Call 1-866-931-6655
Over a century of
providing excellence.


Greenhorne & O'Mara, Inc.
One Team. Infinite Solutions.

Greenhorne & O’Mara is now Stantec. Contact us for coatings and corrosion consulting, design, analysis, and inspection services at john.woods@stantec.com.


Graco Inc.
The Fastest Way
to Touch-Up

The XForce™ HD cordless sprayer for spot repair, small jobs and touch-up. Easily sprays the toughest protective and marine coatings (up to 100% solids).


STOPAQ
Click here if you
Dare to Compare

Permanent Visco-Elastic Corrosion Prevention Traditional systems versus Stopaq Solutions.


LS Industries
LS Blasters: Optimum Steel Cleaning Efficiency

Simplify surface prep with the precise shot control of LS Blasters. Our blast technology delivers optimum coverage and finish. 800-533-8008


US Minerals
US Minerals -
Black Magnum

With nationwide production and distribution capabilities, U.S. Minerals supplies a complete range of coal slag and other abrasives to meet all of your blasting needs.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com