D3322 Standard Practice for Testing Primers and Primer Surfacers Over Preformed Metal

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: June 16, 2011
Updated On: June 28, 2011
Editorial Change:
 
Primers and primer surfacers may be used over many different surfaces top coated with one or more of a variety of coatings and subjected to many kinds of wear and exposure.

The selection of the tests to be used for any given product or system must be governed by experience and by the requirement agreed upon between the producer and the user.

(Back to all Standards)

 
   

US Minerals
US Minerals -
Black Magnum

With nationwide production and distribution capabilities, U.S. Minerals supplies a complete range of coal slag and other abrasives to meet all of your blasting needs.


GMA Garnet USA
GMA Garnet™
Natural Abrasives

- Superior cleaning performance
- Even Profile
- Low Dust
- Cost-Effective
- Environmentally friendly
- Recyclable up to 5 times
Tel : +1 832 243 9300


Graco Inc.
The Fastest Way
to Touch-Up

The XForce™ HD cordless sprayer for spot repair, small jobs and touch-up. Easily sprays the toughest protective and marine coatings (up to 100% solids).


Carboline Company
Hyrdrocarbon Fire & Jet Fire Protection

Pyroclad X1 is the latest breakthrough in epoxy based intumescent fireproofing technology


Harsco
BLACK BEAUTY® GLASS

A 100% post-consumer bottle glass abrasive from a company you can trust. Toll Free: 1-888-733-3646


Oxford Instruments Coating Measurement
Oxford Instruments Coating Thickness Analyzers

Measure paint thickness/protective coatings using Oxford Instruments’ handheld and benchtop gauges, and XRF analyzers. Email industrial@oxinst.com or +1 800-447-4717


Madison Chemical Industries Inc.
Your zinc-rich primer
is obsolete!

Madison’s Zinc-Rich
technology takes the
state of the art to a
new level. AlumiZinc ‘S’
offers superior protection
in a user-friendly
and forgiving format.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com