D331 Standard Specification for 2-Ethoxyethanol

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: June 08, 2005
Editorial Change:
 
1.1 This specification covers 2-ethoxyethanol.

1.2 The values stated in SI units are to be regarded as the standard. No other units of measurement are included in this standard.

1.3 The following applies to all specified limits in this standard; for purposes of determining conformance with this standard, an observed value or a calculated value shall be rounded off "to the nearest unit" in the last right-hand digit used in expressing the specification limit, in accordance with the rounding-off method of Practice E 29.

1.4 For hazard information and guidance, see the supplier's Material Safety Data Sheets.

(Back to all Standards)

 
   

Madison Chemical Industries Inc.
There’s only one CorroCote

Madison invented CorroCote
in 1974 to prevent corrosion
in underground fuel storage
tanks. Today, it’s still the
classic coating for protecting
infrastructure


EDCO - Equipment Development Co. Inc.
EDCO's Quick Response Codes

EDCO now includes Quick Response Code decals on machines. These QRC's provide customers with instant jobsite advice, problem solving tips and much more. Click to watch EDCO machines in action.


International Bridge Conference
International Bridge Conference

Join us in Pittsburgh over June 2-6, 2013 to celebrate the 30th Anniversary of the International Bridge Conference®, the world’s premier technical conference on bridges.


Rapid Prep, LLC
Nation Wide Equipment Rentals

Rapid Prep, LLC is a full service provider of sandblasting & all other surface preparation equipment, with 60 years of experience within the industrial painting industry.


Graco Inc.
The Fastest Way
to Touch-Up

The XForce™ HD cordless sprayer for spot repair, small jobs and touch-up. Easily sprays the toughest protective and marine coatings (up to 100% solids).


Sherwin-Williams
Ask Sherwin-Williams

Does your Paint company know where your Paint is?
If your paint company is Sherwin-Williams it does.
Leave Nothing to Chance


ElektroPhysik
High-precision coating thickness gauge MiniTest 7400

MiniTest 7400 with intuitive menu control, enhanced data management with configuration assistent. Wear-resistant sensors for measuring tasks up to 35mm thickness.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com