SSPC-SP 13/NACE No. 6, Surface Preparation of Concrete

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: March 01, 2003
Updated On: June 01, 2003
Editorial Change: June 1, 2003
 
This standard covers the preparation of concrete surfaces prior to the application of protective coating or lining systems. This standard should be used by specifiers, applicators, inspectors, and others who are responsible for defining a standard degree of cleanliness, strength, profile, and dryness of prepared concrete surfaces.

This standard gives requirements for surface preparation of concrete by mechanical, chemical, or thermal methods prior to the application of bonded protective coating or lining systems. The requirements of this standard are applicable to all types of cementitious surfaces including cast-in-place concrete floors and walls, precast slabs, masonry walls, and shotcrete surfaces.

The requirements of this standard are applicable to all types of cementitious surfaces including cast-in-place concrete floors and walls, precast slabs, masonry walls, and shotcrete surfaces.

(Back to all Standards)

 
   

GMA Garnet USA
GMA Garnet™
Natural Abrasives

- Superior cleaning performance
- Even Profile
- Low Dust
- Cost-Effective
- Environmentally friendly
- Recyclable up to 5 times
Tel : +1 832 243 9300


Cardolite Corporation
CNSL Based Products

Renewable CNSL epoxy curing agents and resins with fast cure at low temperature, adhesion to unprepared surfaces and excellent corrosion and water protection.


PreTox Products - NexTec, Inc.
GOT LEAD? Specify Pretox System products

The ONLY Lead Stabilizer Compatible with All Paint Removal Methods. Works with all Blast Media: Grits | Recyclable Abrasives | CO2 | Water | Power Tools | Etc. Call Dave Steffen at 800.338.8296.


Hempel (USA) Inc.
Real Coating
for Real Protection

Hempel's protective coatings cover a wide range of applications across multiple industries from oil and gas to power generation to infrastructure.


Atlantic Design, Inc.
Rentals, Rentals & More

Our rental fleet has grown and
now includes newer models
with our enhanced safety
features and recent
upgrades. Call today for rates. 866.Call.ADI


Blastox/The TDJ Group, Inc.
Blastox - One Step
Lead Abatement

Don't waste $$ on added labor steps with other methods. Don't mix, meter or apply at the job-site. Avoid strict hazardous waste rules.
Let your painters paint!


Denso North America Inc.
Denso SeaShield
Marine Systems

A full range of steel, concrete and timber pile rehabilitation systems including petrolatum systems, fiberglass jackets, epoxy grouts and many other product lines.
Call 1-281-821-3355 or Visit densona.com

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com