D2794 Standard Test Method for Resistance of Organic Coatings to the Effects of Rapid Deformation (Impact)

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: December 23, 2010
Updated On: February 02, 2011
Editorial Change:
 
Coatings attached to substrates are subjected to damaging impacts during the manufacture of articles and their use in service. In its use over many years, this test method for impact resistance has been found to be useful in predicting the performance of organic coatings for their ability to resist cracking caused by impacts.

1.1 This test method covers a procedure for rapidly deforming by impact a coating film and its substrate and for evaluating the effect of such deformation.

1.2 This test method should be restricted to testing in only one laboratory when numerical values are used because of the poor reproducibility of the method. Interlaboratory agreement is improved when ranking is used in place of numerical values.

(Back to all Standards)

 
   

Fox Industries Inc.
Repair, Protect & Strengthen

Need a coating? Turn to Fox. We have solutions to repair, protect and strengthen concrete, steel and wood substrates. Call 888-760-0369 or email info@foxind.com


JPCL - PCE - PaintSquare
Charter Advertising Opportunities Available through April 30.

Click above or contact Bernadette Landon
Publisher, JPCL Europe blandon@jpcleurope.com +1.412.697.0184
visit www.jpcleurope.com


International Paint LLC
Our New Protective Coatings Centers

Our complete range of International and Devoe Coatings products are available at our Protective Coatings Centers, making purchases faster and easier.


Axxiom Manufacturing
Schmidt Introduces
the New miniBRS

Reduced in size, it is incredibly easy to maneuver and operate! The perfect alternative to larger blast & recovery units when project space is limited.
Call 1-800-231-2085


Van Air Systems
Moisture problems in your air lines?

Van Air Systems' Blast Pak is a portable compressed air drying system that reduces downtime in all blasting and coating applications.


NLB Corporation
Handheld VertaJet™ for concrete or steel

Ergonomic VertaJet from NLB boosts surface prep productivity. Rotating 40,000 psi water jets strip a 6” path and get into corners, with vacuum recovery.


Mascoat
Global Leader In Thermal Insulating Coatings

Our coatings are uniquely engineered and manufactured in-house to fulfill market-specific needs, enhance energy retention, prevent CUI and protect personnel.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com