C1017 Standard Specification for Chemical Admixtures for Use in Producing Flowing Concrete

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: February 15, 2005
Editorial Change:
 
1.1 This specification covers two types of chemical admixtures to be added to hydraulic cement concrete mixtures for the purpose of producing flowing concrete. The types are as follows: 1.1.1 Type I—Plasticizing, and 1.1.2 Type II—Plasticizing and retarding.

1.2 This specification stipulates tests of a chemical admixture with reference concreting materials or with concrete-making materials proposed for specific work. Unless otherwise specified by the purchaser, the tests shall be made using reference concreting materials.

1.3 If a chemical admixture has been tested and found to comply with the provisions of this specification using reference materials, and is being considered for use with other materials for specific work, additional tests for such use are allowed if agreed upon between the purchaser and the supplier and are allowed to consist of a portion of the tests described herein.

1.4 This specification provides for three levels of testing. 1.4.1 Level 1—During the initial approval stage, proof of compliance with the performance requirements defined in demonstrates that the admixture meets the requirements of this specification. Uniformity and equivalence tests of the section on Lot Uniformity and Equivalence shall be carried out to provide results against which later comparisons can be made. 1.4.2 Level 2—Limited retesting described in the section relating to general requirements may be requested at intervals by the purchaser. Proof of compliance with the requirements of demonstrates continued conformity of the admixture with the requirements of the specification. 1.4.3 Level 3—For acceptance of a lot or for measuring uniformity within or between lots, when specified by the purchaser, the uniformity and equivalence tests of the section on Lot Uniformity and Equivalence shall be used.

1.5 The values stated in SI units are to be regarded as standard. The values in inch-pound units shown in parentheses are provided for information purposes only.

(Back to all Standards)

 
   

Safety Lamp of Houston, Inc.
Wet & hazardous area lighting solutions from SAFETY LAMP of Houston

New WOLF LED and fluorescent lights are now available, including low voltage tank lighting kits.
Call: (281) 964-1019.


Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors

Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com


Atlantic Design, Inc.
Your Job Just Got Safer!

In 2013 we've streamlined
many of our products.
They are even more
economical, with enhanced
safety features. All with the same ADI power you expect. 866.Call.ADI


Graco Inc.
The Fastest Way
to Touch-Up

The XForce™ HD cordless sprayer for spot repair, small jobs and touch-up. Easily sprays the toughest protective and marine coatings (up to 100% solids).


Denso North America Inc.
Tank Base Protection

An easy to apply system utilizing Denso tapes and coatings around the tank base, that helps prevent corrosion from external elements.
Call 1-281-821-3355 or Visit densona.com


International Paint LLC
Our New Protective Coatings Centers

Our complete range of International and Devoe Coatings products are available at our Protective Coatings Centers, making purchases faster and easier.


NLB Corporation
Handheld VertaJet™ for concrete or steel

Ergonomic VertaJet from NLB boosts surface prep productivity. Rotating 40,000 psi water jets strip a 6” path and get into corners, with vacuum recovery.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com