TM0304-2004 Offshore Platform Atmospheric and Splash Zone Maintenance Coating System Evaluation

All Standards | NACE Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 24, 2012
Editorial Change:
 
New in 2004. Specifies test methods to evaluate the performance of offshore atmospheric and splash zone maintenance coating systems on platforms, such as fixed-leg, semi-submersible, tension-leg, floating production storage offloading systems (FPSOs). Key words: cathodic protection, galvanic anode CP, impressed CP, offshore platforms, protective coatings, sacrificial anodes

(Back to all Standards)

 
   

Corrosion Specialties, Inc.
The T93R Airless
Tip System

is the longest lasting, highest quality tip and guard available to coatings applicators around the world. Click the link to contact Corrosion Specialties.


Novatek Corporation
Dustless Coatings Removal

Strip it, clean it, and profile it,
all dust free! High production
rates and Blast like finishes.
Comply with new lead
standards.


PreTox Products - NexTec, Inc.
GOT LEAD? Specify Pretox System products

The ONLY Lead Stabilizer Compatible with All Paint Removal Methods. Works with all Blast Media: Grits | Recyclable Abrasives | CO2 | Water | Power Tools | Etc. Call Dave Steffen at 800.338.8296.


Corrosion Probe, Inc.
From Detection to Correction

Corrosion Probe, Inc. has the Most Concrete Coatings Experience and Expertise. Contact us today at
860-767-4402, www.cpiengineering.com


DeFelsko Corporation
NEW PosiTector
Inspection Kits

PosiTector 6000 Coating Thickness Gage easily converts to a surface profile gage, dew point meter or ultrasonic wall thickness gage with a simple probe change.


Safway Services
One Source. Every Solution.

The Safway Group is your source for multiservices. Painting, coating, insulation and more – all from the most trusted name in the industry.


Cardolite Corporation
CNSL Based Products

Renewable CNSL epoxy curing agents and resins with fast cure at low temperature, adhesion to unprepared surfaces and excellent corrosion and water protection.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com