TM0104-2004 Offshore Platform Ballast Water Tank Coating System Evaluation

All Standards | NACE Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 24, 2012
Editorial Change:
 
New in 2004. Specifies test methods to evaluate ballast water tank coatings on offshore platforms, such as tension leg platforms (TLps), semi-submersible platforms, or floating production and storage offloading systems (FPSOs). Key words: coating systems, coating materials, test specimens, offshore platforms.

(Back to all Standards)

 
   

Denso North America Inc.
Tank Base Protection

An easy to apply system utilizing Denso tapes and coatings around the tank base, that helps prevent corrosion from external elements.
Call 1-281-821-3355 or Visit densona.com


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Truss bridge treated with Termarust's (HR CSA) in 1995. This highway & rail truss bridge is still stable and there still is no active corrosion.


Axxiom Manufacturing
Schmidt Improves
Portable Blasters

Schmidt's VBS System reduces blowdown intensity, prevents exhaust from damaging floor while using no screens or filters. Reduces sound; Increasing safety.
Call 1-800-231-2085


LS Industries
LS Blasters: Optimum Steel Cleaning Efficiency

Simplify surface prep with the precise shot control of LS Blasters. Our blast technology delivers optimum coverage and finish. 800-533-8008


Sherwin-Williams
Ask Sherwin-Williams

Does your Paint company know where your Paint is?
If your paint company is Sherwin-Williams it does.
Leave Nothing to Chance


TruQC, LLC
Click here to start your free trial

TruQC is cloud-based job-site documentation built for the iPad. It's easy-to-use, objective and complies to common industry standards. Learn more: TruQCApp.com.


Wasser High-Tech Coatings Inc.
Wasser Coatings

have been used to protect some of the most important bridges in the country; learn about our NEPCOAT-approved system as well as our entire range of MCU coatings and Polyurea membranes.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com