International Paint LLC
 
Are Organic and Inorganic Polymer Concretes an Effective Alternative to Coating Concrete for Maximum Life Expectancy?
| More

By Gary Hall, Sauereisen; Pete Jansen, Sauereisen and Lake Barrett, Sauereisen

Presented at SSPC 2013; Session: Looking Down at Concrete Floor Protection; Session chair: Steve Schroeder

You must sign in to view this presentation.*



*By signing in and accessing the video, you agree to the terms and conditions of this site.

This presentation provides an overview of organic and inorganic polymer concrete technology relative to the common practice of polymer coatings over Portland based concrete. The presentation utilizes an asset management approach and supplements the discussion with actual case studies.