UHP Water Jetting and Surface Tolerant Coatings in New Building Applications

|

By Nuno Cipriano, Narus Consultoria and Joaquim Quintela, Petroleo Brasileiro S.A.

Presented at SSPC 2017; Session: Surface Preparation: The Foundation of Every Coating Project; Session chair: Kevin Irving

You must sign in to view this presentation.*



*By signing in and accessing the video, you agree to the terms and conditions of this site.

After about 20 years of research and development, wet surface tolerant coatings are well established, allowing the expansion of water jetting facilities in both maintenance and new building shipyards. This presentation shares over a decade’s worth of experience using ultra high-pressure hydro blasting and wet surface tolerant coatings on several projects around the world.