What is the best method for removing a day-glo orange spray graffiti from a brick wall?


Selected Answers

From Jerry LeCompte of mmlj on November 10, 2010:
Though not day-glo specifically, the City of Chicago uses soda blasting for graffiti removal.

Please sign in to submit your answer this question    

Tagged categories: Graffiti removal


Current PSF Question | Submit a PSF Question | Full PSF Archive

Rapid Prep, LLC
Nation Wide Equipment Rentals

Rapid Prep, LLC is a full service provider of sandblasting & all other surface preparation equipment, with 60 years of experience within the industrial painting industry.


STOPAQ
Click here if you
Dare to Compare

Permanent Visco-Elastic Corrosion Prevention Traditional systems versus Stopaq Solutions.


3M Corrosion Protection Products
3M™ Sotchkote™ 323 Field Applied Coatings

Let 3M show you how 50 years of experience can lead to less waste, less rework, and more productivity. Our coatings are proudly made in the U.S.A. go.3M.com/Find/Distributor


International Paint LLC
Our New Protective Coatings Centers

Our complete range of International and Devoe Coatings products are available at our Protective Coatings Centers, making purchases faster and easier.


No Ordinary Soda
ARMEX® baking soda-based abrasives from the makers of ARM & HAMMER® products offers over 12 formulas specially engineered for your application and your budget.


Oxford Instruments Coating Measurement
Oxford Instruments Coating Thickness Analyzers

Measure paint thickness/protective coatings using Oxford Instruments’ handheld and benchtop gauges, and XRF analyzers. Email industrial@oxinst.com or +1 800-447-4717


Corrosion Probe, Inc.
From Detection to Correction

Corrosion Probe, Inc. has the Most Concrete Coatings Experience and Expertise. Contact us today at
860-767-4402, www.cpiengineering.com

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com