How can I determine if my urban hospital building would benefit financially by installing a reflective roof coating on top of the current flat black roofing substrate?


Selected Answers

From Darrell Smith of Brown Engineering Comoany on March 11, 2014:
Among the factors that need to be considered are the amount and condition of roof insulation present and the climate zone of your building. The insulation needs to be in good condition and not wet. If the insulation provides the thermal insulating (R) value that is recommended for the climate zone, then application of a reflective coating will be more beneficial in Climate Zones 1 through 4. In Climate Zones 5 through 7,  a more detailed analysis may be required for this determination.

Please sign in to submit your answer this question    

Tagged categories: Roof coatings


Current PSF Question | Submit a PSF Question | Full PSF Archive

DRYCO
The one way to control
a tank: DRYCO

Temporary climate control equipment. Dehumidifiers,
Heaters, A/C, Power, More…
Toll Free: 866-379-2600


Polyval Coatings
POLYFLEX brand Polyurea

high chemical resistant membranes are used extensively to protect our environment in secondary containment applications.


Abrasives Inc.
See the difference immediately Black Magic®

Quality blast abrasive goes farther. Use Black Magic® The Tough Stuff coal slag. Cleaner, consistent, less dust. Order yours today!
Abrasives Inc. 800-584-7524


Sauereisen, Inc.
Experts in Corrosion

A Leader in the manufacture of speciality cements and corrosion-resistant materials of construction. www.sauereisen.com


Mohawk Garnet
Enska by Mohawk Garnet™

A safe, efficient and economical abrasive alternative to slag and sand products. More information
at 1.866.642.7638 or info@mohawkgarnet.com Email for follow up – mheilimo@mohawkgarnet.com


ABKaelin, LLC
Quality is our bottom line

Services include:
• Environmental, Health &
  Safety
• Contractor QP Certification
• Quality Assurance Programs
  and Auditing
• SSPC C3/C5 and other
  Training
• Coatings
• Design/Construction
See our website at abkaelin.com or contact us today abkaelin@comcast.com


Absolute Equipment/Grand Rental Station
Portable Power from Absolute Equipment

•Compressors
•Lighting Systems
•Generators
•Light Compaction
Sales • Rental • Service
Call 1-866-931-6655
Over a century of
providing excellence.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2014, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com