During a week of heavy rain, we painted the interior of a heated concrete building. The paint blistered badly a week later on the walls with an outside exposure. What’s the best way to remove the coating, prepare the surface, and recoat to prevent future blistering?


Selected Answers

From Car F. of Municipal City on December 3, 2013:
Before doing anything on the INSIDE, I would investigate whats on the outside walls and what kind of waterproofing was applied [if any] to the exterior walls. You seem to indicate that the walls NOT facing the outside were fine, so this may point  to a problem related to the exterior walls and not necessarily to the actual coating. Concrete is not impervious, and water and moisture will migrate, sometimes a great distance.

From juan hurtado of International Paint on November 27, 2013:
You can also remove the coating by blasting with with crushed  walnut shells, which is a lot faster than soda blasting.And I would also recommend  checking the concrete for moisture.

From Michael Quaranta of OPERATIONS 40 on November 25, 2013:
Well, for the first element of searching for a response, what kind of coating was used? Probably the heated concrete building was very high in interior humidity, and if you used the standard epoxy, it was doomed for failure. Without knowing what coating was used, it becomes a guess about the best the removal process. Soda blast would be slow but perhaps the best. Next, use a water-based epoxy, and either spray of roll that coating (colors available) on the concrete wall. The pot life is more than 2 hours and the cure is razor-proof after 24 hours.

Please sign in to submit your answer this question    

Tagged categories: Blistering; Coating failure


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
SAFE Systems, Inc.
 
Enduroguard -
The Tough Cable
for a Tough Industry.
 
Reduce maintenance costs and down time, increase job site safety with Enduroguard Cable. Available exclusively from SAFE Systems. UL listed, flexible, abrasion resistant and cut resistant.
 

 
SABRE Autonomous Solutions
 
Safety
 
Removing blasting operators from harmful environments is our key objective.
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
Vector Technologies Ltd.
 
The Original Performance Proven Vacuum Solutions
 
VecLoader® 616 Double Dump, Continuous Vacuum, 170 HP w/ 2,400 CFM & 28” Hg. 33% More Efficient than traditional vacuum systems! Choose Vector for the most powerful and the most reliable trailer mounted vacuums in the industry! Email us at: inquiry@vector-vacuums.com or call us at: 800-832-4010
 

 
Blastox/The TDJ Group, Inc.
 
Blastox® - One Step Lead Abatement
 
Sandblast additive delivered to jobsite pre-blended to eliminate hazardous abrasive wastes. Why mix, meter or apply at the job-site? Blast with ease and
Let your painters paint!
1(800)-252-7869
 

 
SSPC: The Society for Protective Coatings
 
http://www.sspc.org/
 
Join SSPC and Enhance
Your Career !
 

 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
Sauereisen, Inc.
 
SewerGard® 210XHB
 
• 300 mils in a single coat by plural component equipment
• Fast Setting
• 100% Solids Epoxy
• Chemical-resistant barrier for municipal wastewater environments
sauereisen.com
 

 
US Minerals
 
Hit Harder. Clean Faster.
 
Black Diamond abrasive products are the toughest, most effective blasting media and supply the superior power you need to get any job done.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us