During newbuilding, do I have to stripe coat edges if I am using an edge retention primer?



More items for Coating Application


Selected Answers

From FRIDAY OWAJI of DELATTRE BEZONS on September 7, 2013:
Yes stripe coating the edge is the best thing, but the applicator should determine if the spec calls for it.

From Empty Jasson of Hai Phong on February 22, 2013:
     Yes, during newbuilding, stripe coat must be carried out on all edges.

From James Albertoni of CA Department of Water Resources on January 22, 2013:
     Technically, you only have to do what the spec says. If your spec doesn't call for stripe coating, then it is not required. However, it is always a good idea and will prolong the life of the coating.

From Per Gabrielsson of Free Lance Consultations and Inspections on January 22, 2013:
     Yes, of course. Physical forces drive the coating away from edges. Always stripe coat with brush, if possible. Stripe also a few cm's from edges.

From Tom Schwerdt of Texas Department of Transportation on January 24, 2013:
     Best practices would be to stripe-coat the edges. I have seen numerous "edge retentive" primers which had 50% or less thickness at an edge when compared to the flat.

From Atanas Cholakov of ACT on January 23, 2013:
     Per, if this is not highlighted in the coating spec, then RFI needs to be risen to seek clarification. Stripe coat is almost always necessary, but IOZ systems might be exempted. The coating spec insists (rules)... nobody else.

From Atanas Cholakov of ACT on January 21, 2013:
     This question can be best answered from your Coating Spec., pre-job meeting. Assessment of structure complexity and accessibility for spray will be an important step with following highlight on areas to be stripe-coated. The paint supplier's tech. rep's opinion is of importance as well.

From Daniel Liu of APC on February 6, 2013:
     Before the project starts, the application procedure, of course including stripe coating, is normally  fixed, mainly based on the specs, during the pre-job conference. If this point is not required or highlighted in the specs, you can apply the stripe coat where necessary, such as poor manual welds with undercuts, etc. In this case, trust your experience!

From Per Gabrielsson of Free Lance Consultations and Inspections on January 23, 2013:
     Atanas, accessibility for spraying has nothing to do with the need for stripe coating. If you aim to spray an edge, how much paint do you actually have on that? And how much dry spraying of adjacent areas? In shipping we know the limitations of the paint supplier;  this is why WE (the owner's inspectors) have to insist in stripe coatings.

Please sign in to submit your answer this question    

Tagged categories: Edge-retentive Primers; Edges


Current PSF Question | Submit a PSF Question | Full PSF Archive

Commercial Sand Blasting & Painting Ltd.
Reliable Service & Superior Workmanship

We’re ready to meet any of your protective coating and lining needs. We can work on your site or in our facilities, with large shops (60,000 sq ft), 40 acres of yard space, and cranes and forklifts on site.


Novetas Solutions
Number 1 Crushed Glass Abrasive in America!

Manufactured from 100% Recycled Glass.
NO Crystalline Silica,
Beryllium & Arsenic
Great White Metal Finish!
4 plants on Navy QPL
Call us at 866-775-6226


SAFE Systems, Inc.
SAFE Systems'
Blast Lights &
Deadman Switches

Halogen or LED blast lights available with our NEW urethane bumper. Switches available in many colors for color coding your hoses.


Novatek Corporation
Dustless Coatings Removal

Strip it, clean it, and profile it,
all dust free! High production
rates and Blast like finishes.
Comply with new lead
standards.


Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors

Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com


Nationwide Overspray
Profession Overspray Removal Services

The Finest Name in Safe Overspray Removal. We specialize in removing all contaminants from any surface. Family Owned and Operated for 33 years! Fully insured. Satisfaction is guaranteed.


DeFelsko Corporation
The Next Generation PosiTest AT-A

NEW Automatic Adhesion Tester features touch screen, adjustable pull-rate, pull limit, hold times, and nature of fracture/user notes.


Atlantic Design, Inc.
CLICK TO SEE..

what we did to this machine! Let ADI upgrade your machine, extending the life, efficiency, and value. Any make. Like new, but better! 866.Call.ADI


WINOA Group
W Abrasives : Shot Peening Solutions

W Abrasives has developed an exclusive range of products to boost your peening and blasting performances.


HoldTight Solutions Inc.
NO FLASH RUST -
NO CONTAMINANTS

Our HoldTight®102 salt remover & flash rust preventer prevents flash rust by removing surface contaminants. It has no equal; only wannabees.
Contact us for your
nearest distributor.
(800) 319.8802 sales@holdtight.com

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2016, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com