Is the MEK rub test a conclusive test to check the cure of IOZ coatings?

More items for Quality Control


Selected Answers

From Simon Hope of Bilfinger Salamis on January 16, 2013:
     MEK rub test is only subjective as proof of cure for IOZ coatings. The test is only valid for the actual area tested and can only be applied to the whole item by extrapolation of result. Confidence in the result can vary wildly, depending on time, humidity and temperature, as the curing mechanism of IOZ is totally dependent on the integration of water into the silicate precursor to create the matrix to support the metallic zinc. Hence, the best advice is that once touch dry, fresh water washing enhances the cure mechanism. High humidity and water washing will give confidence and MEK rub then gives verification.

From wenbo chen of Morimatsu on January 15, 2013:
     Though ASTM D 4752 describes a standard test method for measuring MEK resistance of IOZ by solvent rub, we always use a coin test in the field. The MEK test is more likely a lab test.

From Chuck Pease of MMI Tank on January 14, 2013:
     Not conclusive, as Dave mentioned. Only a estimation. This requirement is per ASTM D 4752.  Note that in the 4th paragraph, line 2, they call it an estimation.

From Dipesh Vyas of CARBOLINE on February 15, 2013:
     My field expereince reveals that the coin test is the best, easiest,quickest most and reliable test to verify curing of spray- applied IOZ film. The MEK rub test, if not performed by a skilled person, can have misleading  results because spray-applied IOZ always has some loose zinc dust ( overspray), and if not cleaned will react with MEK  In first 5 passes, only satin will be noticed .

From Tom Schwerdt of Texas Department of Transportation on January 22, 2013:
     Wenbo, the MEK rub is certainly a field test - all you need is a rag, MEK and a finger! (Okay, a glove would be nice to have, too.) The MEK rub is more conclusive than the coin test. The only truly conclusive test is in the lab - generally a force cure in a sealed vial, followed by gas chromatography.

From Dave Lisnock of Arizona State University W.P. Carey Facilities on January 14, 2013:
     No, it is not  a conclusive test. The only true test is a lab test.

From Tom Schwerdt of Texas Department of Transportation on February 19, 2013:
     Dipesh - how crisp is the edge of your coin? How much force are you using? At what angle are you holding the coin? The coin test is at least as variable (if not more so) than the MEK rub test.

Please sign in to submit your answer this question    

Tagged categories: Curing; Performance testing


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
DeFelsko Corporation
 
PosiTector SST Soluble Salt Tester
 
Measures the concentration of soluble salts on metal surfaces. Use with all Bresle patch types including the reusable, adhesive-free PosiPatch.
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
SAFE Systems, Inc.
 
Portable Dust Collectors for Tough Environments
 
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.
 

 
KTA-Tator, Inc. - Corporate Office
 
Instrument Service Department
 
Are you a QP certified contractor? KTA’s Instrument Service Department can help keep you compliant!
Click or call 1-800-KTA-GAGE.
 

 
Fischer Technology Inc.
 
FISCHER Expands Corrosion Product Line
 
Rounding out Fischer’s extensive line of products for measuring protective coatings in the corrosion industry is the new ultrasonic wall thickness gauge UMP series.
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
ARC / A.W. Chesterton Company
 
Superior Impact & Wear Resistant Lining
 
100% solids, impact resistant, ceramic reinforced, epoxy/urethane hybrid lining for severe abrasive wear and impact resistance.
 

 
Sauereisen, Inc.
 
SewerGard® 210XHB
 
• 300 mils in a single coat by plural component equipment
• Fast Setting
• 100% Solids Epoxy
• Chemical-resistant barrier for municipal wastewater environments
sauereisen.com
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy (Updated 1/8/2018)   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us