How do you keep sealants in control joints from cracking or separating from the substrate?


Selected Answers

From Ken Johnson of Heritage Preservation on November 29, 2012:
      Proper joint design and substrate preparation are the best solutions. A properly designed joint will not exceed the elasticity to the jointing materials. Surface preparation of the substrate is very important. Sealants will not adequately bond to dust,dirt and moisture that may may lie upon the surface of the substrate. When in doubt, use a primer, even when the manufacturer's data sheet indicates that one is not required.

Please sign in to submit your answer this question    

Tagged categories: Sealers


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
SEMicro Division, M.E. Taylor Engineering, Inc.
 
Coatings Adhesion Testers
 
The PATTI® accurately measures the bond strength between coating & substrate. Outfitted properly, the surface can be rough, porous, or curved & >10K psi strong!
 

 
Safway Services
 
Safeguard Assets. Ensure Productivity. HAKI®
 
Protect assets and equipment. Keep facilities open and operational. Maintain schedules regardless of weather. Ensure smooth and continuous production. Easy to erect. Safway is the primary distributor of HAKI® products including HAKISPAN and HAKITEC® 750 – in North America.
 

 
SAFE Systems, Inc.
 
Portable Dust Collectors for Tough Environments
 
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.
 

 
SABRE Autonomous Solutions
 
Quality
 
The ALPHA1 provides a consistent finish day-in
day-out; job to job.
 

 
International WorkBoat Show
 
Power Forward
 
Join us Nov. 29 – Dec. 1 in New Orleans for the 2017 International WorkBoat Show. If it can power your business forward, you’ll find it here. Register Now!
 

 
Fischer Technology Inc.
 
NEW Protective Coating Inspection Website
 
Click Here!
 

 
Strategic Materials Inc.
 
www.truabrasives.com
 
TruAbrasives™, a clean crushed glass abrasive superior to other abrasives for performance, health, and environmental benefits.
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
Tnemec Company, Inc.
 
Online Coating Courses from Tnemec
 
For decades, Tnemec has offered its expertise to clients presenting face-to-face coatings courses. Now, these presentations are available to anyone for CEUs at Tnemec University.
 

 
Vector Technologies Ltd.
 
The Original Performance Proven Vacuum Solutions
 
VecLoader® 616 Double Dump, Continuous Vacuum, 170 HP w/ 2,400 CFM & 28” Hg. 33% More Efficient than traditional vacuum systems! Choose Vector for the most powerful and the most reliable trailer mounted vacuums in the industry! Email us at: inquiry@vector-vacuums.com or call us at: 800-832-4010
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us