How do I minimize corrosion at the splash zone on sheet pile and piping in brackish water?


Selected Answers

From Doyle Menard of Steel Painters INC on April 6, 2012:
     A good coating to minimize corrosion at the splash zone is International Interzone 954.

Please sign in to submit your answer this question    

Tagged categories: Corrosion


Current PSF Question | Submit a PSF Question | Full PSF Archive

U.S. Zinc

www.USZINC.com


Helping the world work with custom
grades and packaging of zinc
dust, oxide, metal and fines.
U.S. Zinc provides direct shipping
to locations worldwide.


TruQC, LLC
Click here to start your free trial

TruQC is cloud-based job-site documentation built for the iPad. It's easy-to-use, objective and complies to common industry standards. Learn more: TruQCApp.com.


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Truss bridge treated in 2000 with Termarust's (HR CSA) field-proven rust mitigation system chemically stopped corrosion, crevice corrosion & pack rust.


Denso North America Inc.
Tank Base Protection

An easy to apply system utilizing Denso tapes and coatings around the tank base, that helps prevent corrosion from external elements.
Call 1-281-821-3355 or Visit densona.com


3M Corrosion Protection Products
3M™ Sotchkote™ 323 Field Applied Coatings

Let 3M show you how 50 years of experience can lead to less waste, less rework, and more productivity. Our coatings are proudly made in the U.S.A. go.3M.com/Find/Distributor


Blastox/The TDJ Group, Inc.
Blastox - One Step
Lead Abatement

Don't waste $$ on added labor steps with other methods. Don't mix, meter or apply at the job-site. Avoid strict hazardous waste rules.
Let your painters paint!


Greenhorne & O'Mara, Inc.
One Team. Infinite Solutions.

Greenhorne & O’Mara is now Stantec. Contact us for coatings and corrosion consulting, design, analysis, and inspection services at john.woods@stantec.com.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com