Polysiloxane Topcoat Eases Application

Tuesday, July 9, 2013

More items for Coating Materials
More items from North America

Comment | More

A new acrylic polysiloxane topcoat has rolled out to the North American market, International Paint LLC announced.

Interfine 1080 is a low-VOC finish coat in a single-pack formulation designed for industrial and offshore applications that require a high standard cosmetic appearance.

The coating was developed to provide a better aesthetic, environmental and cost-saving alternative to traditional two-pack polysiloxane and polyurethane topcoats, according to the company.

Interfine 1080

Interfine 1080, a new single-pack acrylic polysiloxane topcoat, reduces the chance of mixing error and saves time, International Paint announced.

"With a single-pack product the complexity of mixing part A with part B is removed, thereby reducing the possibility of error," said Dave Maurer, Protective Coatings Senior Product Marketing Manager, North America.

"The easy-to-use formulation will save both time and material costs, while providing exceptional performance and long-term aesthetics," said Maurer.

It does not contain isocyanates and can be applied by brush or roller in several on-site and maintenance applications, such as storage tank externals, pipelines, railings, structural steel and commercial infrastructure.

About the Company

For over 100 years, International Paint has provided protective coatings for customers in the oil and gas, chemical processing, power, mining, heavy duty, commercial and marine industries.

International Paint is part of AkzoNobel, a global supplier of a wide range of paints, coatings and specialty chemicals.

More information: www.international-pc.com.

   

Tagged categories: Acrylic; AkzoNobel; Commercial Buildings; International Paint; Low-VOC; Offshore; Polysiloxane; Single component coatings; Topcoats

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
SABRE Autonomous Solutions
 
Quality
 
The ALPHA1 provides a consistent finish day-in
day-out; job to job.
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
CHLOR*RID International Inc.
 
SOLUTIONS THAT WORK
 
Companies that invest in corrosion control use CHLOR RID products
  • Soluble salt removal liquid
  • Test kits to verify contamination levels
  • Surface passivation to hold the blast
INFO@CHLOR-RID.COM 800.422.3217
 

 
NLB Corporation
 
NLB Sure Shroud: Greater Protection and Flexibility
 
NLB’s Sure Shroud’s lighter weight and flexibility reduces operator fatigue and offers unmatched protection against high pressure hose ruptures. 10k to 40k psi rated.
 

 
Absolute Equipment/Grand Rental Station
 
TIER 4 EQUIPMENT
 
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. www.absoluteequip.com or Call 412-931-6655.
 

 
KTA-Tator, Inc. - Corporate Office
 
Instrument Service Department
 
Are you a QP certified contractor? KTA’s Instrument Service Department can help keep you compliant!
Click or call 1-800-KTA-GAGE.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us