3M Unveils Abrasion-Resistant Epoxy

Tuesday, June 11, 2013

More items for Coating Materials

Comment | More

3M Scotchkote has introduced Abrasion Resistant Epoxy Coating (AREC) 328, a 100% solids, two-part epoxy system designed for directional drilling, rocky terrain, and other rugged applications.

Combining a traditional liquid epoxy with patent pending technology that enables enhanced impact resistance, gouge resistance, and flexibility, an AREC coating can be used in place of a conventional field applied Abrasion Resistant Overcoat (ARO).
 
3M Scotchkote AREC 328

3M says an AREC system is an alternative to a conventional field-applied Abrasion Resistant Overcoat.

3M says the product boasts strong adhesion to both metal and FBE and is effective for use as a primary corrosion protection coating for applications which require high flexibility after cure, in which long-term adhesion is critical.
 
The coating has been formulated to achieve a coating thickness of 45 mils/1150 microns in one coat. If additional thickness is required, additional coats may be applied within four hours of the initial coat at temperature of 70°F/20°C.

The system can be used as a joint coating, a pipe coating or refurbishing coating.

The line consists of 3M Scotchkote Abrasion Resistant Epoxy Coating 328 - 4L, 10L, 68L and 760L.
 
More information: AREC 328.

 

   

Tagged categories: 3M; Abrasion resistance; Epoxy; Pipeline

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
SAFE Systems, Inc.
 
SAFE Systems'
Blast Lights &
Deadman Switches
 
Halogen or LED blast lights available with our NEW urethane bumper. Switches available in many colors for color coding your hoses.
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
ARC / A.W. Chesterton Company
 
Superior Impact & Wear Resistant Lining
 
100% solids, impact resistant, ceramic reinforced, epoxy/urethane hybrid lining for severe abrasive wear and impact resistance.
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
SABRE Autonomous Solutions
 
Productivity
 
Personnel are free to do other tasks while the ALPHA1 does the “dirty work”.
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
Vector Technologies Ltd.
 
The Original Performance Proven Vacuum Solutions
 
VecLoader® 616 Double Dump, Continuous Vacuum, 170 HP w/ 2,400 CFM & 28” Hg. 33% More Efficient than traditional vacuum systems! Choose Vector for the most powerful and the most reliable trailer mounted vacuums in the industry! Email us at: inquiry@vector-vacuums.com or call us at: 800-832-4010
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us