Dur-A-Flex Inc. has expanded its Electro-Static Dissipative floor coating line with the introduction of Armor-Stat ESD.
Armor-Stat is designed to dissipate the static charge caused by the movement of people and high-speed manufacturing and assembly equipment. The coating system can ground out static charges and prevent static events from occurring, Dur-A-Flex says.

The three-step, epoxy-urethane ESD system is designed to provide a durable, seamless, non-porous finish with superior abrasion, UV and chemical resistance and long wear.
Applications include packaging and electronic manufacturing plants; automated and electronic assembly areas; storage areas, clean rooms and AGV warehouses.
Properties, Options
Armor-Stat ESD is available in five colors and has these properties, the manufacturer reports:
• Percent Solids: 70%
• Body Voltage Generation (w/ dissipative footwear), ESD STM 97.2: 14v
• Abrasion Resistance (ASTM D-4060): 5 mg loss
• UV Resistance: Excellent
• Cure Time, Touch Dry at 68° F: 8-10 hours
• Cured Film Thickness: 28 mils
• VOC Content: 10 g/L
• LEED Credit Eligible