Army, Tesla Pioneer Carbon Nanocoating

Wednesday, August 31, 2011

More items for Coating Materials

Comment | More

Super strong, electrically conductive, wear resistant and offering electrostatic discharge protection, carbon nanotubes (CNTs) have long held major potential for structural materials.

Now, an Ohio company and the U.S. Army Corps of Engineers have developed the first commercially available corrosion-resistant coating for steel made with fullerene CNTs.

 Diagram of carbon nanotubes

 Saperaud / Wikimedia Commons

Carbon nanotubes—the research focus of Nobel Laureate Richard Smalley—are long, hollow structures with walls formed by one-atom-thick sheets of graphene.

Teslan Carbon Nanocoating was jointly developed by Tesla NanoCoatings Ltd., of Massillon, OH, and the U.S. Army Engineer Research and Development Center, Construction Engineering Research Laboratory (ERDC-CERL), of Champaign, IL.

Zinc Content Halved

The epoxy polyamide product features about half the zinc content of traditional zinc-rich primers, which protect steel surfaces through the sacrificial action of the zinc dust.

Zinc particles are anodic to steel, and this corrosion protects the steel substrate from corrosion. However, experts say, the high volume of zinc dust pigment (up to 90% by weight) reduces the strength of the coating, increases permeability, and makes delamination of the paint film more likely.

Adding CNTs—long, hollow structures with walls formed by one-atom-thick sheets of graphene—to the formulation allows zinc particles to remain in electric contact, providing as much corrosion protection as before, but without the harmful effects of higher pigment volume content (PVC), researchers say.

The lower pigment load means better adhesion and a stronger barrier film that outperforms barrier-only technology, the developers say. The barrier film is reinforced by the carbon nanotubes and provides corrosion protection via the electrically conductive nanotubes and an optimized amount of anodic metal dust.

Tank Testing

Developers call the nanocoating “the innovative foundation of a complete coating system,” which also includes a compatible polyurethane topcoat.

 Army Corps. of Engineers

 Army Corps of Engineers ERDC CERL

A fuel tank at Fort Bragg is shown before (left) and after application of Teslan, an epoxy and polyurethane coating formulated with carbon nanotubes.

The first test panels were coated at ERDC in 2005, and the coating was first evaluated last year in the field when it was applied to the exterior surfaces of a 200,000-gallon fuel storage tank at Fort Bragg, NC.

Stronger than Steel

In a presentation on the coating, the Corps of Engineers reports that carbon nanotubes can carry 1,000 times the current of copper and boast tensile strength 50 times greater than steel.

CNT research was pioneered by Nobel Laureate Richard Smalley, of Rice University.

The new coating was named a 2011 R&D 100 Winner by R&D Magazine (formerly, Industrial Research).

   

Tagged categories: Barrier coatings; Coatings technology; Corrosion resistance; Epoxy; Nanotechnology; Polyurethane; Protective coatings; Research; U.S. Army Corps of Engineers

Comment from B. BRYCE, (9/2/2011, 4:08 AM)

Does anyone know if there are additional health & welfare requiremets when using these materials eg can the very small nano particles pass through traditioanl PPE & human membranes?


Comment from Richard McLaughlin, (9/6/2011, 9:52 AM)

Bryce, the short answeris "yes", there are health concerns with nano-sized particles, but that concern should be greatly reduced or eliminated once the particles are placed in a suspension, like a coating, or in a finished product. Concerns about worker exposure to nanoparticles come up on several safety email list I read, like the one hosted be the University of Vermont. Some nanoparticles can pass through most PPE and in some cases right straight through a worker’s skin due to the particle’s size. Many can pose a danger to a worker’s internal organs, with lung damage being the most common concern. By the way, man-made nanoparticles are nothing new, just the variety is. We’ve been making carbon black and fumed silica for a very long time and they fall into the “nanoparticle” category. You’ve safely interacted with nanoparticle containing products every time you’ve changed a tire or dealt with a reinforced plastic product. Like I said, once in a suspension or finished product, nanoparticles are normally safe.


Comment Join the Conversation:

Sign in to our community to add your comments.

Sherwin-Williams
Ask Sherwin-Williams

Does your Paint company know where your Paint is?
If your paint company is Sherwin-Williams it does.
Leave Nothing to Chance


BASF
New resins from BASF will have metals loving water:

Excellent corrosion resistance, low VOC, high gloss, thin films basf.us/industrialcoatings
polyorders@basf.com
800-231-7868


Wasser High-Tech Coatings Inc.
Wasser Coatings

have been used to protect some of the most important bridges in the country; learn about our NEPCOAT-approved system as well as our entire range of MCU coatings and Polyurea membranes.


Versaflex Inc.
Best NSF 61.5 Approved Potable Water Polyurea

VersaFlex Polyurea Earns Highest ANSI/NSF 61.5 Rating for High Temp Service, Minimum Tank Size and Max Thickness. All Polyureas Are Not Created Equal. FREE WHITE PAPER.


SSPC: The Society for Protective Coatings
http://www.sspc.org/

Join SSPC and Enhance
Your Career !


ANAFAPYT (Asociación Nacional de Fabricantes de Pinturas y Tintas)
ANAFAPYT Latin American
Coatings Show 2013

You are still on time to sign up
for Conferences, Exhibit Floor
and Short Course. Be part of
the best show in Latin
America. www.lacs2013.com


DeFelsko Corporation
NEW PosiTector
Inspection Kits

PosiTector 6000 Coating Thickness Gage easily converts to a surface profile gage, dew point meter or ultrasonic wall thickness gage with a simple probe change.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com