Goad Company is introducing custom-engineered tank linings for companies with critical containment requirements and/or concerns about leaks.
The linings incorporate Goad’s patented TANKeye leak detection system, which is designed to locate leaks electronically, without draining the tank and without the need for intrusive spark testing, the company reports.

Goad Tank Linings use Koroseal flexible PVC sheets and employ RF-welded panels. They are constructed with N-FUZE Lining Technology (patent pending), which features molded corner inserts and infused machine welds that are designed to eliminate gaps resulting from imperfect hand welds.
Varied Containment Applications
Goad says the linings may be used with virtually any type of containment, tank or pit, with linings and coatings such as epoxies, fiberglass, rubber, Belzona, Ceilcote, Flakeline, Heresite, and Plasite.
Linings are priced according to configuration, construction and application. Price quotations are provided upon request.

Established in 1955, St. Louis-based Goad Company provides custom-designed tank linings, fabrications and systems to the surface finishing and chemical process industries. Goad also offers a comprehensive corrosion-resistant fabricating service, including lining and coatings application.
More information: http://www.goadco.com/.
|