DOD Turns Lights, Camera, Action on Corrosion Training

Friday, May 13, 2011

More items for Program/Project Management

Comment | More

The Defense Department is trying to recruit new troops of all ages in its war on corrosion, with several new programs in development for today’s and tomorrow’s engineers.

For current professional engineers, DOD’s Office of Corrosion Policy and Oversight  (CorrDefense) is developing a series of free, online training videos that will highlight 15 areas of concentration related to corrosion and materials degradation.

Several segments are planned for each area, and all will be technical, polished, professional-level presentations, written by CorrDefense and aimed at working engineers who would benefit from corrosion training, says CorrDefense director Daniel J. Dunmire.

 DOD Office of Corrosion Policy and Oversight

 DOD Office of Corrosion Policy and Oversight

DOD’s Corrosion Office wants to train engineers, and turn on students, to the field of materials degradation.

“There are so many engineers out there who know nothing about corrosion, who never heard of corrosion during their education,” says Dunmire, who is passionate about corrosion education.

Beyond Talking Heads

“This has never been done before, and certainly hasn’t been done for free,” Dunmire said in an interview. “We’re writing the scripts from scratch. They won’t just be talking heads. We’re trying to keep them compelling to watch.”

The corrosion engineering content will have a military focus, but nearly all of the information is transferable to civilian applications, Dunmire says.

“Materials are materials are materials, and they all degrade,” he said.

Each segment will take one to three hours to work through, and CorrDefense hopes to have the first one—an overview of corrosion engineering issues—available on its site by January.

‘These Will Last’

The project will incorporate guidelines and parameters set by Defense Acquisition University, which offers training and professional development for the defense acquisition workforce.  The videos are being produced by Bruno White Entertainment Inc., whose clients also include Disney and Coca-Cola.

The cost of the project is not yet known, but it should be a one-time expense; the content should have an unlimited shelf life, Dunmire says.

“Unless there’s some new physics from God, these things will last,” he said. “We’re making sure these will last.”

Reaching Tomorrow’s Engineers

Professional development is one thing; trying to make material degradation sexy to young people choosing a career path is another.

“The biggest problem we have in corrosion is that we do not have enough people in the field,” Dunmire says. “We have such a lack of excitement in the field of material degradation. And we want to show that this is an exciting field.”

To that end, the agency is heading an initiative to develop an interactive middle-school-oriented exhibit to bring the science of corrosion and materials degradation to school students.

Working with representatives of SSPC, NACE, the NACE Foundation and Bruno White Entertainment, CorrDefense is developing a model display for the Orlando Science Center, which draws about 80,000 school-aged visitors each year.

“This is a brand-new initiative, and the people involved are going to make it happen,” Dunmire says. Group members have been surveying local science center displays and programs since their initial meeting a few months ago; they meet next on May 26.

Private Investment Sought

Dunmire hopes the initial exhibit, which his organization will fund, will become a prototype that private industry can then customize, replicate and export to other science centers at far less expense. The goal is to install such exhibits at every science center in the country.

The prototype will cost about $80,000, and subsequent exhibits could probably be developed for about half that cost, Dunmire estimates.

“This is very important,” he says. “I’m hoping we’ll have a pipeline of kids who at least know what corrosion is, and remember that when they go to college. If I get one [student to pursue a career in the field], it pays for itself.” 

   

Tagged categories: Coatings education; Corrosion protection; NACE; SSPC; Worker training

Comment from Jim Deardorff, (5/16/2011, 4:51 AM)

Dan, Jim Deardorff here,I remember talking to you several years ago about my work. I would like to offer my help in developing training videos for the large percentage of people that have corrosion problems but, don't have access to corrosion training. Since 2005, I have been featured on RFD-TV "The Farm Station" as the "Paint Professor" offering advice on how to help fight rust and corrosion for farm equipment and facilities. I have also been writing new articles on my Lifetime Coating System Concept which also has the potential to save energy. Like you, I realize that a large percentage of facility owners don't have access to current painting standards. It time to make corrosion prevention technologies available to a wider range of coating users. Jim Deardorff Superior Coatings


Comment from David Hunter, (5/16/2011, 7:35 AM)

Dan: How may I contact you regarding the above?


Comment from Mary Chollet, (5/16/2011, 9:06 AM)

Dan Dunmire can be reached at Daniel.Dunmire@osd.mil.


Comment from Tom Schwerdt, (5/23/2011, 8:24 AM)

Sounds great! I hope there will be another article when the first video is available.


Comment Join the Conversation:

Sign in to our community to add your comments.

PPG Protective and Marine Coatings Group
Industrial strength performance in ONE can.

Now get the durability and protection of two components in one can: Amercoat® ONE, PSX® ONE and Sigmadur ONE.


Ethox Chemicals LLC
Ethoflex® ER instantly upgrades your epoxy!

The only epoxy additive that improves flexibility, corrosion resistance, toughness, and adhesion, without hurting pot life, cure time, or increasing VOCs.


SSPC: The Society for Protective Coatings
http://www.sspc.org/

Join SSPC and Enhance
Your Career !


Chicago Corrosion Group
Vendor-neutral corrosion consulting

Give us a $1 and we’ll save you $10.
For more information,
call 877-516-9514


Mitsubishi Gas Chemical America
Performance Amine 1,3-BAC

A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.


Hempel (USA) Inc.
HEMPEL PROTECTIVE COATINGS

Efficient systems and high quality products to reduce your maintenance costs. Visit Hempel Protective for more information.


Midsun Specialty Products
Stopaq 30+ Year Coatings

Use Stopaq corrosion prevention coatings on pipelines, field joints, tank chimes, structural steel and more. Learn more at www.midsunsp.com/stopaq


Sherwin-Williams
Sherwin-Williams Protective & Marine Coatings

With 4,000 distribution points and 3,700+ years of experience, Sherwin-Williams delivers the products, support and expertise you need, right where you need it.


SAFE Systems, Inc.
Enduroguard -
The Tough Cable
for a Tough Industry.

Reduce maintenance costs and down time, increase job site safety with Enduroguard Cable. Available exclusively from SAFE Systems. UL listed, flexible, abrasion resistant and cut resistant.


Specialty Products, Inc. (SPI)
SIGN UP TODAY – HANDS ON TRAINING

After 40 years in the coating business, SPI has trained more industry professionals than any other polyurea manufacturer. Now offering more classes at more locations than ever before!

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2015, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com