New NASA Coating is Blacker than Black

Friday, December 10, 2010

More items for Coating Materials

Comment | More

John Hagopian

Black is black, right? Not so, according to a team of NASA engineers now developing a blacker-than-pitch material that will help scientists gather hard-to-obtain scientific measurements and observe currently unseen astronomical objects.

The nanotech-based material now being developed by a team of 10 technologists at the NASA Goddard Space Flight Center in Greenbelt, MD, is a thin coating of multi-walled carbon nanotubes—tiny hollow tubes made of pure carbon about 10,000 times thinner than a strand of human hair.

Nanotubes have a multitude of potential uses, particularly in electronics and advanced materials, due to their unique electrical properties and extraordinary strength. But in this application, NASA is interested in using the technology to help suppress errant light that has a funny way of ricocheting off instrument components and contaminating measurements.

‘Better than Black Paint’

"This is a technology that offers a lot of payback," said engineer Leroy Sparr, who is assessing its effectiveness on the Ocean Radiometer for Carbon Assessment (ORCA), a next-generation instrument designed to measure marine photosynthesis. "It's about 10 times better than black paint" typically used by NASA instrument designers to suppress stray light, he said.

The technology works because of its super-absorption abilities. The nanotubes themselves are packed vertically much like a shag rug. The tiny gaps between the tubes absorb 99.5% of the light that hits them. In other words, very few photons are reflected off the carbon-nanotube coating, which means that stray light cannot reflect off surfaces and interfere with the light that scientists actually want to measure. The human eye sees the material as black because only a small fraction of light reflects off the material.

The team began working on the technology in 2007. Unbeknownst to the group, the New York-based Rensselaer Polytechnic Institute also had initiated a similar effort and announced in 2008 that its researchers had developed the darkest carbon nanotube-based material ever made—more than three times darker than the previous record.

"Our material isn't quite as dark as theirs," said John Hagopian, the principal investigator leading the development team. "But what we're developing is 10 times blacker than current NASA paints that suppress system stray light. Furthermore, it will be robust for space applications.”

That is an important distinction, said Carl Stahle, assistant chief of technology for Goddard's Instrument Systems and Technology Division. Not all technology can be used in space because of the harsh environmental conditions encountered there.

"That's the real strength of this effort," Stahle said. "The group is finding ways to apply new technology and fly it on our instruments."

Big Breakthrough

The breakthrough was the discovery of a highly adhesive underlayer material upon which to grow the carbon nanotubes, which are just a few tens of nanometers in diameter. To grow carbon nanotubes, materials scientists typically apply a catalyst layer of iron to an underlayer on the silicon substrate. They then heat the material in an oven to about 750° C (1,382° F). While heating, the material is bathed in carbon-containing feedstock gas.

Stephanie Getty, the materials scientist on Hagopian's team, varied the underlayer as well as the thickness of the catalyst materials to create carbon nanotubes that not only absorb light, but also remain fixed to the material upon which they are grown. As a result, they are more durable and less likely to scratch off. The team also has grown durable nanotube coatings on titanium, a better structural material for space use. The team now is fine-tuning production techniques to assure consistent quality and light-suppression capabilities, Hagopian said.

New Capabilities Added

Should the team prove the material's suitability in space, the material would provide real benefits to instrument developers, Hagopian added.

Currently, instrument developers apply black paint to baffles and other components to reduce stray light. Because reflectance tests have shown the coating to be more effective than paint, instrument developers could grow the carbon nanotubes on the components themselves, thereby simplifying instrument designs because fewer baffles would be required.

To accommodate larger components, the team now is installing a six-inch furnace to grow nanotubes on components measuring up to five inches in diameter. And under a NASA R&D award, the team also is developing a separate technique to create sheets of nanotubes that could be applied to larger, non-conforming surfaces.

   

Tagged categories: Coatings technology; Protective coatings; Research

Comment Join the Conversation:

Sign in to our community to add your comments.

International Paint LLC
New! Chartek

The next evolution in passive fire protection has arrived! Check out our new line of Chartek products.


BASF
New resins from BASF will have metals loving water:

Excellent corrosion resistance, low VOC, high gloss, thin films basf.us/industrialcoatings
polyorders@basf.com
800-231-7868


Carboline Company
Fireproofing Solutions

Pyroclad® X1 Thermo-Lag® Pyrocrete® – protecting against hydrocarbon and jet fires, explosions, and cryogenic spills.


Wasser High-Tech Coatings Inc.
Wasser Coatings Protect

Wasser Coatings offer a complete range of Moisture Cure Urethane (NEPCOAT approved) systems in addition to Polyurea membranes and linings(NSF).
www.wassercoatings.com


SSPC: The Society for Protective Coatings
http://www.sspc.org/

Join SSPC and Enhance
Your Career !


Binks/DeVilbiss
Built for Tough Jobs

From Epoxies to Urethanes to other high solid coatings, the new Binks Airless 75 delivers a great finish using an ergonomic design. Visit binks.com for more information.


Thermion Inc
Buy Back Program

We are offering $5,000
credit for your old Model
This drive system is
being discontinued by
the manufacturer.
More information at
thermioninc.com
877.884.3428


Polyval Coatings
Polyflex® Polyurea Linings

Polyflex™ new Polyurea Geotextile Membrane System has been specifically engineered to protect the environment in containment applications.
www.polyflexlinings.com


Mitsubishi Gas Chemical America
Performance Amine 1,3-BAC

A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.


Jessup Manufacturing Company
More Traction for Extreme Marine Conditions

Jessup Safety Track® 3800 Military Grade peel-and-stick non-skid tapes and treads provide extra slip resistance for decks. MIL-PRF-24467C Type XI, Black & Gray.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2015, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com