New PPG Coating Passes Navy’s Muster

Tuesday, September 14, 2010

Comment | More

PPG Industries’ protective and marine coatings  business has introduced PSX 700SG for use by U.S. Navy vessels and other federal marine coatings applications.

The new product is a semi-gloss version of PPG’s patented PSX 700 epoxy polysiloxane coating and has been engineered to meet and exceed marine coating requirements established by the U.S. government, PPG says.

PSX 700SG is approved on the U.S. Navy Qualified Product List (QPL) for topside and freeboard applications and meets the U.S. Navy Federal Standard Color standards for Haze Gray. PSX 700SG also complies with U.S. Department of Defense MIL-PRF-24635E, Type V (high-durability), Type VI (high-durability, low-volatile organic compound), Class 2 (semi-gloss), Grade B (low solar-absorbing) specifications.

Cost Savings

PSX 700SG can reduce the total operating cost of government vessels, according to Steve Feldman, PPG national sales director, protective coatings, North America. “In addition to its low-VOC formulation, PSX 700SG has unlimited recoatability, making touch-up and maintenance easier while being a color-stable LSA (low solar-absorbing) coating,” Feldman said.

PSX 700SG is designed to provide superior abrasion resistance, wide cure-temperature flexibility and surface tension that minimizes rust or dirt streaking.

To learn more, visit www.ppgpmc.com/northamerica or call 1-888-9PPGPMC (977-4762).

Other PPG Protective and Marine Coatings brands include Amercoat and Sigma Coatings.

   

Tagged categories: Marine; Marine Coatings; PPG; U.S. Navy

Comment Join the Conversation:

Sign in to our community to add your comments.

JPCL - PCE - PaintSquare
Charter Advertising Opportunities Available through April 30.

Click above or contact Bernadette Landon
Publisher, JPCL Europe blandon@jpcleurope.com +1.412.697.0184
visit www.jpcleurope.com


Clemco Industries Corp.
Powerful Protection in a Small Package

Mounts inside blast helmet, alerts operator to dangerous breathing-air condition by audible, visual, and vibratory alarms. Easily calibrated, battery operated.


Oxford Instruments Coating Measurement
Oxford Instruments Coating Thickness Analyzers

Measure paint thickness/protective coatings using Oxford Instruments’ handheld and benchtop gauges, and XRF analyzers. Email industrial@oxinst.com or +1 800-447-4717


SAFE Systems, Inc.
Enduroguard -
The Tough Cable
for a Tough Industry.

Reduce maintenance costs and down time, increase job site safety with Enduroguard Cable. Available exclusively from SAFE Systems. UL listed, flexible, abrasion resistant and cut resistant.


Axxiom Manufacturing
Revolutionary Units

By integrating Schmidt's Aftercoolers with our blast pots, these systems remove moisture from air and minimize equipment footprint on jobsite.
Call 1-800-231-2085


International Paint LLC
Our New Protective Coatings Centers

Our complete range of International and Devoe Coatings products are available at our Protective Coatings Centers, making purchases faster and easier.


Van Air Systems
The Blast Pak

Van Air Systems' portable desiccant air dryer. Get dry compressed air with this All-In-One blasting and coating solution.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com