SSPC Issues Guide to Evaluating Flash Rust

Tuesday, April 27, 2010

Comment | More

SSPC issued a guide to performance of a field assessment of flash rust, “Recommended Guidelines for Evaluating Flash Rust.”

The publication is described as a “non-mandatory guide” with text and reference describing how to perform a field assessment of the amount of flash rust on a steel surface by brushing the surface with a paint brush wrapped with a white cotton cloth. The assessment involves an evaluation of the color and amount of rust that transfers to the cloth.

SSPC said the guide was developed for the National Shipbuilding Research Program Surface Preparation and Coatings Panel (NSRP SP-3).

The guide is available for $50 for SSPC members and $60 for non-members. To order: www.sspc.org/marketplace.

   

Tagged categories: Corrosion protection; Flash rusting; Protective coatings; SSPC

Comment Join the Conversation:

Sign in to our community to add your comments.

Hempel (USA) Inc.
Real Coating
for Real Protection

Hempel's protective coatings cover a wide range of applications across multiple industries from oil and gas to power generation to infrastructure.


SSPC: The Society for Protective Coatings
http://www.sspc.org/

Join SSPC and Enhance
Your Career !


Mascoat
Global Leader In Thermal Insulating Coatings

Our coatings are uniquely engineered and manufactured in-house to fulfill market-specific needs, enhance energy retention, prevent CUI and protect personnel.


ANAFAPYT (Asociación Nacional de Fabricantes de Pinturas y Tintas)
ANAFAPYT Latin American
Coatings Show 2013

You are still on time to sign up
for Conferences, Exhibit Floor
and Short Course. Be part of
the best show in Latin
America. www.lacs2013.com


Blastox/The TDJ Group, Inc.
Blastox - One Step
Lead Abatement

Don't waste $$ on added labor steps with other methods. Don't mix, meter or apply at the job-site. Avoid strict hazardous waste rules.
Let your painters paint!


Denso North America Inc.
Tank Base Protection

An easy to apply system utilizing Denso tapes and coatings around the tank base, that helps prevent corrosion from external elements.
Call 1-281-821-3355 or Visit densona.com


International Paint LLC
Our New Protective Coatings Centers

Our complete range of International and Devoe Coatings products are available at our Protective Coatings Centers, making purchases faster and easier.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com