SSPC Issues One New Standard, Revises Second

Monday, August 7, 2017

Comment | More

SSPC: The Society for Protective Coatings has released one new standard—moisture determination on commercial coating projects—and revised another, pertaining to polyurethanes.

Guide to Moisture Determination

The new publication, SSPC Guide 23, Field Methods for the Determination of Moisture in Concrete and Masonry Walls and Ceilings, EIFS and Stucco, is a guide describing five common field methods of determining moisture content in certain exterior walls. The methods can be used on painted and unpainted concrete and masonry walls (including concrete masonry units, brick, stone, poured-in-place, pre-cast and tilt-up), Exterior Insulation and Finish Systems and stucco, and concrete and masonry ceilings.

Coated brick wall
© / marimashi

Guide 23 describes five common field methods of determining moisture content in substrates including painted and unpainted concrete and masonry walls (including concrete masonry units, brick, stone, poured-in-place, pre-cast and tilt-up).

The new guide includes generic descriptions of equipment used in measuring moisture content, conditions necessary to perform testing, test procedures and other considerations affecting test results. It was developed by SSPC C.8.1 Commercial Cleaning and Painting, a committee chaired by Kevin Brown, of KTA-Tator Inc.

Polyurethane Lab Testing Standard

The revised standard is SSPC Paint 41, Moisture-Cured Polyurethane Primer or Intermediate Coat, Micaceous Iron Oxide Reinforced, Performance-Based. This standard provides lab testing benchmarks and acceptance criteria for generic coating type in its title. It was revised by SSPC C.1.3.D Polyurethane Coatings Committee, chaired by Michael J. Masciale.

The revision involves an expansion of the scope of the standard, which now allows for the moisture-cured polyurethane primer to be used either as a direct-to-steel coating or as an intermediate coat over a compatible primer.

Paint 41 has also been revised in relation to standard testing conditions, requirements of liquid coating, laboratory testing of applied coatings and scribe evaluation.

The new standard and the newly revised standard are both available via the SSPC Marketplace or via the SSPC App.

Founded in 1950, SSPC is the only nonprofit association that is focused on the protection and preservation of concrete, steel and other industrial and marine structures and surfaces through the use of high-performance protective, marine and industrial coatings.


Tagged categories: Certifications and standards; Laboratory testing; Moisture detection; Moisture-cured polyurethane; Primers; SSPC; Testing + Evaluation

Comment Join the Conversation:

Sign in to our community to add your comments.

DeFelsko Corporation
PosiTector SST Soluble Salt Tester
Measures the concentration of soluble salts on metal surfaces. Use with all Bresle patch types including the reusable, adhesive-free PosiPatch.

Fischer Technology Inc.
Maximize Profits by Monitoring Coating Thickness
Learn more by contacting Fischer Technology today: 1.860.683.0781

KTA-Tator, Inc. - Corporate Office
KTA-Tator EH&S Services
• Ambient & Worker Exposure Air Monitoring
• Safety & Health Program Development
• Lead Paint Assessments
& Specifications
• Health Hazard & Jobsite Safety Assessments
Call 1-800-532-3633

SSPC: The Society for Protective Coatings
Join SSPC and Enhance
Your Career !

HoldTight Solutions Inc.
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802

Mitsubishi Gas Chemical America
Performance Amine 1,3-BAC
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.

Blastox/The TDJ Group, Inc.
Blastox® - One Step Lead Abatement
Sandblast additive delivered to jobsite pre-blended to eliminate hazardous abrasive wastes. Why mix, meter or apply at the job-site? Blast with ease and
Let your painters paint!

Tarps manufacturing, Inc.
QUALITY MADE IN AMERICA —Available near you!
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.

Absolute Equipment/Grand Rental Station
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. or Call 412-931-6655.

SAFE Systems, Inc.
Portable Blast &
Recovery Equipment
Trailer or skid mounted blast and recovery equipment. Systems designed for maximum versatility, environmental compliance
and overall cost savings.
Call 1-800-634-7278


Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL

The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us