Friday, March 31, 2017

Comment | More

Coatings manufacturer Axalta Coating Systems (Philadelphia) has introduced two new products to its Nap-Gard line of pipeline coatings.

Nap-Gard 7-0017HT and 7-0017VHT FBE Black Beauty are thermosetting epoxy powders that Axalta says are designed to provide chemical resistance at temperatures up to 392 degrees Fahrenheit. The internal pipeline coatings are designed to fight corrosion caused by carbon dioxide and hydrogen sulfate, often found in sour crude oil.

Internal pipeline coating

Axalta says its two new Nap-Gard internal pipeline coatings provide chemical resistance at temperatures up to 392 degrees Fahrenheit.

Both new powders diiffer from the already-existing Nap-Gard 7-0017 product in that they are capable of withstanding higher temperatures.

In addition to internal FBE coatings, Axalta’s Nap-Gard line of products also includes external pipe coatings, rebar coatings, valve coatings and girth weld coating and FBE repair materials.

More information:


Tagged categories: Axalta; Epoxy; Industrial powder coating; Pipeline; Powder coatings; Single-layer FBE

Comment Join the Conversation:

Sign in to our community to add your comments.

Carboline Company
New product: Carbozinc® 608 HB
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!

New resins from BASF will have metals loving water!
Excellent corrosion resistance, low VOC, high gloss, thin films 800-231-7868

SABRE Autonomous Solutions
Removing blasting operators from harmful environments is our key objective.

Tarps manufacturing, Inc.
QUALITY MADE IN AMERICA —Available near you!
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.

HoldTight Solutions Inc.
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802

Mitsubishi Gas Chemical America
Performance Amine 1,3-BAC
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.

Jotun Paints Inc.
Jotun Jotachar 1709
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.

Bullard Made in the USA

Fischer Technology Inc.
FISCHER Expands Corrosion Product Line
Rounding out Fischer’s extensive line of products for measuring protective coatings in the corrosion industry is the new ultrasonic wall thickness gauge UMP series.

Absolute Equipment/Grand Rental Station
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. or Call 412-931-6655.


Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL

The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us