Resin Made to Up Coating Performance

Monday, August 15, 2016

Comment | More

Silicone chemistry company SiVance LLC, a subsidiary of Milliken & Company, has introduced a new reactive silicone technology designed to create highly durable epoxy-silicone hybrid coating formulations.

SiVance C2010 resin is described as a high-performance material that helps extend the flexibility and impact resistance of protective coatings used in harsh operating environments such as undersea drilling, hydraulic fracturing and chemical manufacturing.

According to the Spartansburg, SC, company, hybrid formulations featuring this new resin enables formulators to help their customers avoid the cracking, delamination and blistering that lead to corrosion and failure of metal pipes, tanks and equipment.

SiVance mandrel test
SiVance LLC

SiVance reports a mandrel bend test comparison, after five days at 120 degrees Celsius (240 degrees Fahrenheit), showed that the control sample (left) cracked and delaminated while the SiVance C2010 resin sample (right) passed.

“While epoxies for protective coatings have been enhanced over the years, they are approaching their limits,” said Jeff Jones, SiVance business development director. “At the same time requirements for today’s extremely demanding environments are escalating.”

Durability in Harsh Conditions

Jones explains that the resin product provides formulators a new tool for extending the durability of epoxies under the harshest of conditions in order to help their end customers reduce maintenance, replacement costs and downtime.

To facilitate formulation of these hybrids, SiVance C2010 resin uses a proprietary structure that makes it broadly compatible with aliphatic epoxies and aromatic epoxies such as bisphenol-A, bisphenol-F and phenol novolacs, the company says.

Coatings formulated with an epoxy-silicone hybrid offer increased durability in highly demanding applications, such as immersion coatings, tank linings, thermal insulation and subsea coatings, the company explains.

It suggests that the resin can benefit industry processes such as oil and gas exploration and extraction, offshore and marine operations and chemical manufacturing.

Flexibility, Impact Resistance

According to the manufacturer, laboratory tests that subjected coatings to high temperatures and pressures showed that a bisphenol-A epoxy-silicone hybrid formulation made with SiVance C2010 resin surpassed a bisphenol-A epoxy formulation in flexibility (conical mandrel bend test and a three-point bend test) and reverse impact performance (ASTM D2794).

These improvements in flexibility and impact resistance were achieved with only a minor decrease in other critical properties, including hardness and glass transition temperature, and had little to no impact on adhesion, SiVance explains.

Although organic modifiers and other reactive silicones provide similar flexibility upon curing, they lose this property more rapidly than the new resin under exposure to demanding environmental extremes, the company adds.

The new C2010 resin is available globally in commercial quantities and is currently registered under the Toxic Substances Control Act (TSCA) with other global approvals in progress, SiVance says.

More information: millikenchemical.com/sivance/.

   

Tagged categories: Coating chemistry; Durability; Epoxy; Formulating; Hybrids; Milliken; Resins; Silicone

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Novatek Corporation
 
Dustless Coatings Removal
 
Novatek Corporation, Dustless Coatings Removal Strip, clean and profile all dust free! Comply with new lead standards. Contact today: (866) 563-7800 www.Novatekco.com
 

 
SABRE Autonomous Solutions
 
Quality
 
The ALPHA1 provides a consistent finish day-in
day-out; job to job.
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
ARC / A.W. Chesterton Company
 
Chemical Resistant Lining
 
ARC S7 is a sprayable, novolac vinyl ester based, ceramic particle reinforced, protective coating for high temperature, chemical exposures where erosive particulates and thermal cycling conditions may be present. ARC S7 can be easily applied by brush, roller or airless spray system.
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
Carboline Company
 
Carboline launches new website!
 
The completely revamped website, offers quick and easy access to essential product information and is now mobile-friendly.
 

 
Sauereisen, Inc.
 
Substrate Repair Materials
 

Substrate Repair Materials and Filler Compounds

Sauereisen's full line of underlayments are the ideal substrate repair materials to restore structural integrity prior to the application of SewerGard©
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us