Advancing Anti-Reflective Coatings

Wednesday, June 15, 2016

Comment | More

A European research institute has put its efforts behind developing an application-specific coating process for anti-reflective coatings that could benefit a range of glass surfaces.

The Fraunhofer Institute for Organic Electronics, Electron Beam and Plasma Technology FEP, which develops innovative solutions in the fields of vacuum coating, surface treatment and organic semiconductors, has tested a new technology for creating anti-reflective coatings on glass, a solar technology news site reported.

The Dresden, Germany-based organization was scheduled to present its latest results at the International Conference on Coatings on Glass and Plastics (ICCG) 2016, June 12-16, in Braunschweig, Germany.

Anti-Reflective Glass

From windshields and solar cell to windows and eyewear, a variety of manufactured products require anti-reflective coatings that allow the glass surfaces to remain crystal clear.

Fraunhofer FOP anti-reflective coating
Fraunhofer FEP

Researchers at Fraunhofer FEP have tested a novel technology for creating anti-reflective coatings on glass.

Solar cells, in particular, benefit from these coatings because they enable the cells to capture nearly all the sunlight that falls on them when the surface inhibits its reflection.

Application of these coatings to substrates like plastic films and rigid or flexible glass, however, can pose a challenge, Fraunhofer FEP says. The coating process needs to be economical while also matching the properties of the layers to the purpose of the specific application, it adds.

Fraunhofer FEP puts its scientific know-how and industrial facilities to work by partnering with clients to develop specialized anti-reflective coatings that meet their specific applications.

Sputtering and Etching

In particular, Fraunhofer FEP researchers are now sharing the new method they have developed to create anti-reflective coatings on glass.

First, a co-sputtering process is used to put down a gradient layer of silicon dioxide (SiO2) and a supplementary component, they say. An etching process then removes the supplementary component, leaving behind a layer of rough silicon dioxide.

“Thanks to the resultant continuous transition in optical properties from air to glass, anti-reflective behavior is exhibited by the surface of the glass,” Solar Novus writes.

The effect is said to be similar to a process FEP uses for making plastic sheets or web anti-reflective. Developed jointly with the Fraunhofer Institute for Applied Optics and Precision Engineering IOF and industrial partners, that process nanoetches the surface of polymers directly with plasma.

“The gradual transition in refractive index from air to polymer achieved this way is likewise anti-reflective,” the technology site explains.

Conventional vs. New Coating

In a conventional anti-reflective coating, layers of high and low refractive index are deposited alternately, the scientists note, which confines the anti-reflective effect to a restricted wavelength. The wavelength’s range can only be broadened through a complex system of interfering layers.

However, an anti-reflective coating system that utilizes the effects caused by rough surfaces is not restricted by wavelength, the researchers explain. Reflection is inhibited over a wide spectral range in a single layer of coating or a single plasma etching step, according to the team.

“The layers achieved with the new process are characterized by a good mechanical durability and the reduction of reflections over a wide spectral range,” explains Thomas Preußner, Fraunhofer FEP researcher for large-area in-line processing told ChemEurope.

Anti-reflective coatings are just one potential application for the co-sputtering method. Fraunhofer FEP scientists see future uses in making battery and solar-cell electrodes larger and more effective, they say.

   

Tagged categories: Coatings; Coatings Technology; Glass; Reflectance; Research and development; Solar; Solar energy; Solar reflectance; Windows

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
SAFE Systems, Inc.
 
Portable Dust Collectors for Tough Environments
 
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
SABRE Autonomous Solutions
 
Quality
 
The ALPHA1 provides a consistent finish day-in
day-out; job to job.
 

 
ARC / A.W. Chesterton Company
 
Superior Impact & Wear Resistant Lining
 
100% solids, impact resistant, ceramic reinforced, epoxy/urethane hybrid lining for severe abrasive wear and impact resistance.
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
Carboline Company
 
Carboline launches new website!
 
The completely revamped website, offers quick and easy access to essential product information and is now mobile-friendly.
 

 
Bullard
 
Upgrade with the Bullard GenVX
 
Click here for your blast helmet.
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us