Free Webinar Focuses on Vapor Blasting

Friday, April 3, 2015

Comment | More

Using water to suppress airborne dust during abrasive blasting can achieve the same power as dry blasting, according to an upcoming webinar.

The results of using a blasting method that adds water to the pressure pot will be covered in "Differences Between Traditional Sandblasting and Vapor Abrasive Blasting," a free upcoming JPCL/SSPC webinar to be held from 11 a.m. to noon ET April 8.

The webinar will be presented by Bill Eliason, a sales manager for Graco and founder of EcoQuip Inc.

Graco EcoQuip

This webinar will cover the science behind vapor abrasive blasting and which types of applications are better suited for this method.

The webinar is part of the 2015 JPCL/SSPC Webinar Education Series.

What You'll Learn

This webinar will discuss the differences between vapor abrasive blasting technology and dry-blasting, slurry-blasting and traditional water-based blasting methods.

Attendees will learn the science behind vapor abrasive blasting and which types of applications are better suited for this method.

Participants may register here free.

This webinar is sponsored by Graco.

About the Presenter

Bill Eliason is a NACE Level II Certified Coatings Inspector and the founder of EcoQuip Inc., which was acquired by Graco in December 2013.

He is currently the North American Sales Manager for the Graco EcoQuip Vapor Abrasive Blast Equipment product line.

Free Webcasts Available

Numerous free webcasts in the JPCL/SSPC Education Series, covering a wide range of topics, are now available at

Spider Staging

Those presentations include:

A complete listing of PaintSquare's archived and future webinars is available here.


Tagged categories: Abrasive blasting; Certifications and standards; Coatings education; Dust Collectors; Graco; JPCL; Oil and Gas; Regulations; SSPC; Webinars; Worker training

Comment Join the Conversation:

Sign in to our community to add your comments.

NLB Corporation
NLB Sure Shroud: Greater Protection and Flexibility
NLB’s Sure Shroud’s lighter weight and flexibility reduces operator fatigue and offers unmatched protection against high pressure hose ruptures. 10k to 40k psi rated.

Graco Inc.
Graco EcoQuip 2: Experience the Difference
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit to learn more.

Tarps manufacturing, Inc.
QUALITY MADE IN AMERICA —Available near you!
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.

Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors
Vacuum and dust collector hose, filters and related accessories.

Jotun Paints Inc.
Jotun Jotachar 1709
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.

HoldTight Solutions Inc.
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802

CHLOR*RID International Inc.
Companies that invest in corrosion control use CHLOR RID products
  • Soluble salt removal liquid
  • Test kits to verify contamination levels
  • Surface passivation to hold the blast
INFO@CHLOR-RID.COM 800.422.3217

SSPC: The Society for Protective Coatings
Join SSPC and Enhance
Your Career !

Mitsubishi Gas Chemical America
Performance Amine 1,3-BAC
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.

ARC / A.W. Chesterton Company


Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL

The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us