Spray Fights Multimetal Corrosion

Monday, November 10, 2014

More items for Coating Materials
More items from North America

Comment | More

Cortec Corp. has rolled out an environmentally friendly, temporary coating designed to protect metals in indoor, outdoor and salt-spray environments.

Water-based VpCI-389 is designed to protect up to five years indoors and six to 24 months in unsheltered, outdoor settings.

Typical applications include aluminum, steel, cast iron, copper alloy and tin-plated steel substrates in overseas shipping, parts storage, equipment lay-up, parts processing and maintenace repairs.

Cortec VpCI-389
Cortec Corp.

Applications include multiple metal substrates in shipping, parts and equipment storage, and maintenance.

Cortec calls VpCI-389 "completely safe and easy to use." The coating cures to a soft film and eventually hardens.

Features, Testing

Traditional coatings rely on sacrificial metals (zinc, chromates, aluminum) for inhibition, Cortec notes.

"Due to the large particle size of these inhibitors, gaps exist which allow corrosion to start and eventually expand, causing coating failure," the company says.

Cortec VpCI-389 is designed with a tight bonding molecular structure that eliminates those gaps, the company says.

Cortec calls the low-VOC product efficient in SO2 and H2S environments and easy to remove with alkaline cleaners.

VpCI-389 coating has been tested according to ASTM D-1748 (humidity chamber test) and ASTM B-117 (salt spray chamber test) and complies with RoHS requirements, the manufacturer says.

More information: www.cortecvci.com.

   

Tagged categories: Aerosol coatings; Aluminum; Cast iron; Corrosion protection; Cortec; Marine; Steel

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
SABRE Autonomous Solutions
 
Introducing the ALPHA1 Blasting Robot
 
Once installed and commissioned – simply
SCAN PLAN BLAST.
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
KTA-Tator, Inc. - Corporate Office
 
Instrument Service Department
 
Are you a QP certified contractor? KTA’s Instrument Service Department can help keep you compliant!
Click or call 1-800-KTA-GAGE.
 

 
SAFE Systems, Inc.
 
Portable Dust Collectors for Tough Environments
 
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.
 

 
ARC / A.W. Chesterton Company
 
Superior Impact & Wear Resistant Lining
 
100% solids, impact resistant, ceramic reinforced, epoxy/urethane hybrid lining for severe abrasive wear and impact resistance.
 

 
SSPC: The Society for Protective Coatings
 
http://www.sspc.org/
 
Join SSPC and Enhance
Your Career !
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us