PPG Adds Steel Intumescent Coatings

Tuesday, July 29, 2014

More items for Coating Materials

Comment | More

PPG Protective & Marine Coatings has announced new products in the Steelguard range of intumescent fire protection coatings for steel structures.

Steelguard 701/801 was developed to target 30- and 60-minute fire scenarios with lower film thicknesses on I-section beams and solid columns, PPG says.

Steelguard 702 was designed for application on hollow sections, for fire scenarios up to 90 minutes.

Steelguard Diagram
PPG

PPG's new Steelguard coatings provide fire protection for hollow and solid steel building components.

Fire Protection

The coatings range is intended to deliver fire protection for civil buildings and can be used on structures where exposed steel is part of the design, such as shopping centers, airport terminals, sports stadiums and schools, according to PPG.

The company says that fast-drying primers and a specially designed topcoat enable three coats to be applied in one day.

The coatings can be left externally exposed for 12 months without top coating, as long as they are not subjected to ponding, running water or immersion, according to PPG.

More information: www.ppg.com.

   

Tagged categories: Airports; Commercial Buildings; Exposure conditions; Fire-resistive coatings; Intumescent; PPG; Stadiums/Sports Facilities; Steel

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
 

 
Novatek Corporation
 
Dustless Coatings Removal
 
Novatek Corporation, Dustless Coatings Removal Strip, clean and profile all dust free! Comply with new lead standards. Contact today: (866) 563-7800 www.Novatekco.com
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
Fischer Technology Inc.
 
TSA Coatings on Stainless Steel
 
Fischer’s Phascope PMP10 and ESD20TSA probe are incredibly accurate and easy to use.
 

 
ARC / A.W. Chesterton Company
 
HT-S
 
ARC HT-S is a 100% solids glass/ceramic reinforced novolac epoxy lining for high temperature aqueous cold wall corrosion conditions. ARC HT-S is easily applied by roller, brush, squeegee, or airless spray.
 

 
Absolute Equipment/Grand Rental Station
 
TIER 4 EQUIPMENT
 
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. www.absoluteequip.com or Call 412-931-6655.
 

 
NLB Corporation
 
NLB Sure Shroud: Greater Protection and Flexibility
 
NLB’s Sure Shroud’s lighter weight and flexibility reduces operator fatigue and offers unmatched protection against high pressure hose ruptures. 10k to 40k psi rated.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us