Metal Gauge Has New Data Capabilities

Monday, June 23, 2014

More items for Quality Control

Comment | More

A new metal thickness gauge from Dorset, England-based Tritex NDT boasts the ability to store readings in grid and string format directly on the tool.

The Multigauge 5700 Datalogger Metal Thickness Gauge takes all the features of the company's Multigauge 5600 and adds the ability to store readings on the tool.

Tritex
Tritex NDT

The Multigauge 5700 Datalogger has onboard memory to store readings, as well as all of the features of the 5600 model.

The 5700 Datalogger includes an onboard memory for recording measurements in either a grid or string format, or a combination of both, the company says. The readings can be transferred to a computer using wireless technology, which also allows remote gauging.

The company says the gauge's software includes wizards to guide the user in setting up templates or files for various applications.

Probe, Measurement Features

The gauge uses the "Multiple Echo" technique to ignore coatings up to 6mm thick and only measures the metal substrate, according to Tritex. No grinding or removal of the coatings is required.

All of the gauge's probes have Intelligent Probe Recognition, which the company says automatically adjust settings in the gauge when connected to match the probe and gauge. The single crystal probes are protected by a membrane so prevent easily being damaged.

The 5700 Datalogger also has the Automatic Measurement Verification System to display only true measurements, even on heavily corroded materials, according to Tritex.

According to the company, the gauge comes ready-to-use with a three-year warranty and free lifetime calibration.

More information: www.tritexndt.com.

   

Tagged categories: Metals; Meters and gauges; Quality control; Thickness gauge; Tools

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
DeFelsko Corporation
 
PosiTector SST Soluble Salt Tester
 
Measures the concentration of soluble salts on metal surfaces. Use with all Bresle patch types including the reusable, adhesive-free PosiPatch.
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
SABRE Autonomous Solutions
 
Quality
 
The ALPHA1 provides a consistent finish day-in
day-out; job to job.
 

 
SAFE Systems, Inc.
 
Portable Dust Collectors for Tough Environments
 
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.
 

 
KTA-Tator, Inc. - Corporate Office
 
Instrument Service Department
 
Are you a QP certified contractor? KTA’s Instrument Service Department can help keep you compliant!
Click or call 1-800-KTA-GAGE.
 

 
Fischer Technology Inc.
 
FISCHER Expands Corrosion Product Line
 
Rounding out Fischer’s extensive line of products for measuring protective coatings in the corrosion industry is the new ultrasonic wall thickness gauge UMP series.
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
North Dakota State University
 
Coatings Science Short Course – Registration Open
 
North Dakota State University, June 10 – 15, 2018. The course is designed for all levels of scientists and technologists working in the field of coating.
 

 
Vector Technologies Ltd.
 
The Original Performance Proven Vacuum Solutions
 
VecLoader® 616 Double Dump, Continuous Vacuum, 170 HP w/ 2,400 CFM & 28” Hg. 33% More Efficient than traditional vacuum systems! Choose Vector for the most powerful and the most reliable trailer mounted vacuums in the industry! Email us at: inquiry@vector-vacuums.com or call us at: 800-832-4010
 

 
SSPC: The Society for Protective Coatings
 
http://www.sspc.org/
 
Join SSPC and Enhance
Your Career !
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us