Concrete Disbonds on New ‘Stan Span’

Wednesday, June 11, 2014

More items for Program/Project Management

Comment | More

A four-month-old, $667 million bridge over the Mississippi River has already undergone repairs, after several areas failed to bond to the deck panel.

According to media reports, the Missouri Department of Transportation was performing permanent repairs in May on the Stan Musial Veterans Memorial Bridge when crews noticed a spot where the two-inch concrete overlay wasn't bonding with the 10-inch concrete underdeck.

MoDOT project director Randy Hitt told local CBS affiliate KMOX that it's not unusual for a bridge of that size to have a few issues.

Stan Musial Veterans Memorial Bridge
Images: Facebook / New Mississippi River Bridge

Crews had to resurface disbonded concrete on about eight square feet of the Stan Musial Veterans Memorial Bridge. The $667 million bridge opened in February.

The 1,500-foot-long cable-stayed bridge opened Feb. 9. The bridge carries two lanes of I-70 in each direction over the Mississippi River between Missouri and Illinois.

'Minor' Repairs

The sections of disbonded concrete accounted for "maybe eight square feet out of roughly 30,000 square feet of deck, so in the grand scheme of things, it's very minor," Hitt told KMOX.

"There's always going to be some issue like an oil spill or it may not have been cleaned perfectly," Hitt said.

Workers discovered the issue while working on the bridge May 19 and 20. The concrete was removed and replaced over a two-night period, according to the St. Louis Post-Dispatch.

According to Hitt, the contractor will be responsible for paying for the repairs performed by MoDOT.

The concrete/latex mix used on the surface was designed for quick repairs and resurfacing, and the surface is designed to last "decades" before needing a complete resurfacing, KMOX reported.

Fight for the Naming Right

The Stan Musial Veterans Memorial Bridge was named for both St. Louis Cardinals icon Stan "The Man" Musial and the nation's veterans.

The 1,500-foot-long cable-stayed bridge was named for St. Louis Cardinals legend Stan Musial and the nation's veterans.

Musial, a career-long Cardinal and a legend in St. Louis, MO, died in January 2013. Weeks later, a proposal to name the new bridge in his honor was well underway in the state Legislature. That measure would have named part of the bridge for Musial and part for Andy Gammon, 35, a local construction worker who fell to his death on the project.

The plan was derailed in Illinois, however, where the state House voted 109-0 to name the span the Veterans Memorial Bridge.

In the end, the decision fell to Congress, because the project is receiving $240 million in federal funds.

   

Tagged categories: Bridges; Concrete defects; Department of Transportation (DOT); Disbondment

Comment Join the Conversation:

Sign in to our community to add your comments.

SAFE Systems, Inc.
SAFE Systems'
Blast Lights &
Deadman Switches

Halogen or LED blast lights available with our NEW urethane bumper. Switches available in many colors for color coding your hoses.


Armakleen Company, The
ARMEX when nondestructive cleaning is critical

The gentle physical propriety of baking soda but yet aggressive cleaning ability is what makes ARMEX the only choice for nondestructive abrasive blasting.


US Minerals
US Minerals -
Black Magnum

With nationwide production and distribution capabilities, U.S. Minerals supplies a complete range of coal slag and other abrasives to meet all of your blasting needs.


HoldTight Solutions Inc.
NO FLASH RUST -
NO CONTAMINANTS

Our HoldTight®102 salt remover & flash rust preventer prevents flash
rust by removing surface contaminants. It has no equal; only wannabees.
Contact us for your
nearest distributor.
(800) 319.8802 sales@holdtight.com


Ethox Chemicals LLC
Ethoflex® ER instantly upgrades your epoxy!

The only epoxy additive that improves flexibility, corrosion resistance, toughness, and adhesion, without hurting pot life, cure time, or increasing VOCs.


PPG Protective and Marine Coatings Group
Industrial strength performance in ONE can.

Now get the durability and protection of two components in one can: Amercoat® ONE, PSX® ONE and Sigmadur ONE.


Minerals Research & Recovery

HIGH PERFORMANCE ABRASIVES


“Made in the USA!”

Why recycle waste from other countries? Go FASTER, CLEANER, at 1/3 THE COST with MR&R “All-American” Sharpshot®HP!!

WATCH THE VIDEO


Abrasives Inc.
Check our Prices for Blast Abrasives

Faced with higher abrasive costs? We invite you to call & check our rates on Black Magic® coal slag and other quality blast materials. Abrasives Inc. 800-584-7524


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Pipeline Utility Aerial crossings coated since 1992. Termarust's (HR CSA) was used to overcoat lead paint and preserve cables, pipes and support towers.


Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors

Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2015, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com