‘Smart Concrete’ May Outlive Us All

Friday, April 11, 2014

More items for Coating Materials

Comment | More

What are you doing in April 2134?

If Scott Muzenski has his way, his great-great-great grandchildren will be doing the very first repairs on the driveway he just patched.

Muzenski, a civil engineering doctoral student at the University of Wisconsin-Milwaukee (UWM), is hoping that his new high-performance concrete composite can pull off a 120-year service life without maintenance.

That would be about three times the current life span for concrete roads in Wisconsin. And that's an average. About 10 percent of reinforced bridge decks need replacement after just 30 years, the university says.

Scott Muzenski and Konstantin Sobolev
Troye Fox / UW-Milwaukee

Dr. Konstantin Sobolev (right) and doctoral student Scott Muzenski work on a sample of the "smart" concrete composite that they believe could last more than 120 years.

The new cement composite being developed in the lab of associate professor Konstantin Sobolev is a durable, water-resistant, malleable paving material with such a high degree of crack control that researchers say it may last 120 years. Or more.

SECC Slab

Sobolev's team is putting the hybrid material—officially, a Superhydrophobic Engineered Cementitious Composite (SECC)—to the test in a university parking structure.

A driveway of the structure had developed a large crack after many Wisconsin winters, making it the perfect testing ground for the material being developed in Sobolev's lab.

Last summer, Muzenski led a crew of 25 students in laying down a 4-by-15-foot slab of their SECC material.

And because they expect the slab to outlive them, the researchers are equipping it with a self-monitoring system.

The students embedded electrodes in the concrete that are linked to a data acquisition system located behind an adjacent retaining wall, the university reported in a research announcement this week.

Tales of Water and Stress

“This is going to tell us whether water is getting into the material and how deep it goes,” Muzenski said in the announcement.

“It also detects the presence of chloride ions within the material, and senses load and stress as vehicles pass over it.”

UW-Milwaukee

Researchers at UW-Milwaukee offer a quick peek at their "concrete that's built to last."

When the software is completed later this year, the real-time data will be fed wirelessly to an online repository, where the team can "observe the performance of concrete as it happens, in real time,” says Sobolev.

Beading and Stretching

The material's secret? There are two, researchers say.

First, its superhydrophobic quality makes water bead up rather than sink into it. An additional tweak of the material at the molecular level gives the hardened concrete a microscopic spiky surface so that the water rolls off from the slightest angle.

Second, the composite's malleability allows it to bend without breaking. Although malleable concrete is not new, the university says Sobolev's lab has improved the material's ductility (stretchiness) by incorporating "super-strong unwoven polyvinyl alcohol fibers."

"When cracks begin, the fibers keep them from becoming larger tears," the university said.

Smaller Cracks

No, the university reports, the goal is not to prevent cracking. It is to force the load and stress across many tiny cracks that will not allow water in—unlike conventional, brittle concrete, where cracks get progressively worse with constant loading.

Cracked bridge
kingcounty.gov

Researchers suggest that the relatively expensive hybrid composite might be best used on areas like bridge approaches, where deterioration typically begins.

“Our architecture allows the material to withstand four times the compression with 200 times the ductility of traditional concrete,” says Sobolev.

Because the ductile concrete is more expensive than traditional concrete, Sobolev recommends that it be used strategically in places where deterioration begins, such as bridge approaches.

That’s where heavily reinforced concrete meets regular asphalt. The joint, says Sobolev, cannot withstand the continuous loading.

“The bridge and the road aren’t designed to work together,” he says. “You need something between them that has the durability to handle the stress.”

If the concrete proves as smart as researchers think, it could have other applications. Sobolev notes, for example, that remote monitoring would be possible at nuclear power plants and other high-risk facilities.

   

Tagged categories: Bridge/parking deck waterproofing; Concrete; Concrete defects; Concrete repair; Concrete slab waterproofing; Cracks; Maintenance programs; Research

Comment from Jerry Trevino, (4/11/2014, 12:31 PM)

This is an extreme noble objective to develop a cementitious material that is more ductile, crack resistant, and impermeable than standard ready mix concrete. These have been the goals of many scientists, chemists and formulators. I strongly believe in formulating and applying unique and specific formulations for specific applications. Although it is said concrete is not rocket science, I do believe that is could be and equal a challenge to develop, and use specific formulations for specific applications. When specifiers do not have intimate knowledge and vast experience in material science, and specify simply a ready mix formulation and only highlight the compressive strength of the concrete and nothing else, durability suffers and the concrete given the blame. Concrete and most construction materials are not that smart, the specifiers need to be the smart ones. This comment is not to diminish the hard work and results of the SECC product. I am extremely hopeful improvements can and will be made. Lets just make sure specifiers apply it in the correct application so that it can last 120 years.


Comment from GERRY WELDER, (5/4/2014, 7:51 AM)

Be ready for your product to get ignored, here’s why: This new product will mean SUBSTANTIALLY LESS MAINTENANCE, LONGER LIFE and must include the biggest eventual cost savings (our taxes) of all - less need for unions/administration/pensions + their uniforms, + equipment/maintenance + fuel costs + cost of arbitrations and negotiations, dealing with all their constant complaints (time is money >taxes<) and their use of massive tax funding levered to contributions to the democrat ELECTIONS. The unions and their democrat puppets will fight this like scorned women.


Comment Join the Conversation:

Sign in to our community to add your comments.

Polyval Coatings
Polyflex® Polyurea Linings

Polyflex™ new Polyurea Geotextile Membrane System has been specifically engineered to protect the environment in containment applications.
www.polyflexlinings.com


BASF
New resins from BASF will have metals loving water:

Excellent corrosion resistance, low VOC, high gloss, thin films basf.us/industrialcoatings
polyorders@basf.com
800-231-7868


Sherwin-Williams
Sherwin-Williams Protective & Marine Coatings

With 4,000 distribution points and 3,700+ years of experience, Sherwin-Williams delivers the products, support and expertise you need, right where you need it.


International Paint LLC

International Paint Engineered Coatings

Learn about our solutions for:
  • Structural Steel
  • Piping & Equipment
  • Storage Tanks
  • Pressure Vessels
  • Secondary Containment


    Jessup Manufacturing Company
    More Traction for Extreme Marine Conditions

    Jessup Safety Track® 3800 Military Grade peel-and-stick non-skid tapes and treads provide extra slip resistance for decks. MIL-PRF-24467C Type XI, Black & Gray.


    Wasser High-Tech Coatings Inc.
    Wasser Coatings Protect

    Wasser Coatings offer a complete range of Moisture Cure Urethane (NEPCOAT approved) systems in addition to Polyurea membranes and linings(NSF).
    www.wassercoatings.com


    Mitsubishi Gas Chemical America
    Performance Amine 1,3-BAC

    A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.


    Carboline Company
    Hydrocarbon Fire & Jet Fire Protection

    Pyroclad X1 is the latest breakthrough in epoxy based intumescent fireproofing technology


    Corrosion Probe, Inc.
    From Detection to Correction

    Corrosion Probe, Inc. has the Most Concrete Coatings Experience and Expertise. Contact us today at
    860-767-4402, www.cpiengineering.com


    HoldTight Solutions Inc.
    NO FLASH RUST -
    NO CONTAMINANTS

    Our HoldTight®102 salt remover & flash rust preventer prevents flash
    rust by removing surface contaminants. It has no equal; only wannabees.
    Contact us for your
    nearest distributor.
    (800) 319.8802 sales@holdtight.com

  •  
     
     
    Technology Publishing

    The Technology Publishing Network

    The Journal of Protective Coatings & Linings (JPCL) PaintSquare
    Durability + Design Paint BidTracker

     
    EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
    REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
    MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
     

    © Copyright 2000-2015, Technology Publishing / PaintSquare, All rights reserved
    2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com