Concrete Waterproofer Made for Extremes

Friday, April 4, 2014

More items for Coating Materials

Comment | More

A new cold-applied waterproofing compound from W.R. Meadows can suit concrete applications in a variety of settings—horizontal and vertical, interior and exterior, below- and above-grade, in heat and cold, the company says.

Hydralastic 836 is a one-component, solvent-free waterproofing material that will not crack in extreme cold or soften and slump at high temperatures, according to the manufacturer.

waterproofing
W.R. Meadows

Hydralastic 836 is a one-component waterproofing membrane that skins over in 30 minutes without dust pickup, according to W.R. Meadows.

The company says Hydralastic 836 can be used for positive-side waterproofing for foundations and between-slab applications.

Additional Features

“It bonds to both concrete and asphalt, does not require primer, will not harm EPS or Styrofoam materials, and there’s no mixing required,” said Brent Weber, W.R. Meadows’ vice president of sales.

The low-VOC product skins over in 30 minutes; will not shrink or freeze; and cures to form a tough, flexible waterproofing membrane, the manufacturer says.

Based in Hampshire, IL, W.R. Meadows Inc. designs, manufactures, and markets building materials for construction professionals. The family-owned and -operated company sells products through an authorized distribution network.

More information: www.wrmeadows.com.

   

Tagged categories: Below grade waterproofing; Concrete slab waterproofing; Construction; W.R. Meadows Inc.; Waterproofing; Waterproofing membranes

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
Detail Masters
 
Overspray Removal
 
We offer professional, turnkey service and unparalleled quality!
Our process can save hundreds— even thousands of dollars. It's fast, environmentally safe and 100% guaranteed.
 

 
SEMicro Division, M.E. Taylor Engineering, Inc.
 
Coatings Adhesion Testers
 
The PATTI® accurately measures the bond strength between coating & substrate. Outfitted properly, the surface can be rough, porous, or curved & >10K psi strong!
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
Monti Tools, Inc.
 
BRISTLE BLASTER® – THE ORIGINAL ONE
 
  • Abrasive blast with a power tool
  • Remove corrosion, mill scale and coatings
  • Cleans & roughens
  • Meets SSPC-SP 10 / NACE No. 2
  • Profile up to 4.7 mils
  • ATEX Zone 1
  •  

     
    SSPC: The Society for Protective Coatings
     
    http://www.sspc.org/
     
    Join SSPC and Enhance
    Your Career !
     

     
    Sauereisen, Inc.
     
    SewerGard® 210XHB
     
    • 300 mils in a single coat by plural component equipment
    • Fast Setting
    • 100% Solids Epoxy
    • Chemical-resistant barrier for municipal wastewater environments
    sauereisen.com
     

     
    Tarps manufacturing, Inc.
     
    QUALITY MADE IN AMERICA —Available near you!
     
    CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
     

     
     
     

    Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

    TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


    The Technology Publishing Network

    Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

     
    EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
    REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
    MORE:      About PaintSquare.com   |   Privacy policy (Updated 1/8/2018)   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us