Duplex Coatings on Kentucky Transportation Cabinet Bridges

From JPCL, January 2017

More items for Coating Materials

By Bobby Meade, Greenman-Pedersen Inc.; and Sudhir Palle and Theodore Hopwood II, University Of Kentucky

Bridges have been historically designed for a theoretical 50-year service life but in many cases remain in service in excess of 75 years. This article discusses one tool that bridge designers can employ to extend bridge coating service life — the use of hot-dip galvanizing (HDG) and duplex coatings....


(Login to read the full article)

   

Tagged categories: Bridges; Duplex coatings; Galvanized steel; Greenman-Pedersen, Inc.; Hot-dip galvanizing; Kentucky Transportation Cabinet

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
SAFE Systems, Inc.
 
Portable Dust Collectors for Tough Environments
 
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
SABRE Autonomous Solutions
 
Repeatability
 
The ALPHA1 provides reliable results consistently allowing you to cost your next job with confidence.
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
International Bridge Conference
 
Bridge conference 2018
 
Registration for the 2018 IBC is now open! Join us in June for the biggest and best IBC ever! View the Program, Workshops and Exhibitors by clicking in the banner.
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
Fischer Technology Inc.
 
DUALSCOPE®FMP100 with DataCenter IP
 
Transfer customized inspection plans from PC to FMP100 using step-by-step guidance with prompts and pictures throughout the measurement procedure
 

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us