New Technology Coatings for Corrosion Control

Relining Potable Water Tanks: Research and Field Work

From JPCL, May 2012

More items for Coating Materials

by R.A. Francis, Ph.D., Aurecon; G. Mattioli, Mattioli Bros.; and S. Smith, Melbourne Water

The authors discuss the issues involved in selecting a tank lining that provides the required strength and flexibility as well as resistance to and compatibility with potable water. The article describes types of linings studied for a tank lining project in Australia and describes the project....
(Login to read the full article)

   

Tagged categories: Coating selection; Corrosion; Linings; Maintenance coating work; Tank interiors; Water Tanks

Comment Join the Conversation:

Sign in to our community to add your comments.

Sherwin-Williams
Ask Sherwin-Williams

Does your Paint company know where your Paint is?
If your paint company is Sherwin-Williams it does.
Leave Nothing to Chance


BASF
New resins from BASF will have metals loving water:

Excellent corrosion resistance, low VOC, high gloss, thin films basf.us/industrialcoatings
polyorders@basf.com
800-231-7868


Versaflex Inc.
Best NSF 61.5 Approved Potable Water Polyurea

VersaFlex Polyurea Earns Highest ANSI/NSF 61.5 Rating for High Temp Service, Minimum Tank Size and Max Thickness. All Polyureas Are Not Created Equal. FREE WHITE PAPER.


Wasser High-Tech Coatings Inc.
Wasser Coatings

have been used to protect some of the most important bridges in the country; learn about our NEPCOAT-approved system as well as our entire range of MCU coatings and Polyurea membranes.


U.S. Zinc

www.USZINC.com


With multiple locations,
ample capacity and a
proven safety record, U.S.
Zinc offers supply security
to customers around the globe.


International Paint LLC
Our New Protective Coatings Centers

Our complete range of International and Devoe Coatings products are available at our Protective Coatings Centers, making purchases faster and easier.


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Hydro Utility Penstock Overcoated in 1997. Was power washed and overcoated with major cost saving. No environmental impact with Termarust's low LC50 of 41,007 ppm.

 
 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com