Issues That Do Not Meet The Eye: Design Considerations for Lining Concrete Sludge Mixing and Storage Tanks in Wastewater Treatment Plants

From JPCL, March 2012

More items for Quality Control

by R.A. Nixon, Corrosion Probe, Inc.

"This article focuses on several condition assessment and design considerations associated with protective linings for corrosion protection in concrete sludge storage and mixing tanks at wastewater treatment facilities. The author shares lessons he has learned through 15 years of field experience performing coating failure analyses at wastewater plants."...
(Login to read the full article)

   

Tagged categories: Concrete; Wastewater Plants

Comment from mahmoud ahmed, (4/26/2012, 1:13 PM)

thanks


Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
DeFelsko Corporation
 
PosiTector SST Soluble Salt Tester
 
Measures the concentration of soluble salts on metal surfaces. Use with all Bresle patch types including the reusable, adhesive-free PosiPatch.
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-Tator Training Course Opportunities
 
• IACET Authorized Continuing Education Unit (CEU) Provider
• Live Basic Coatings Inspection Courses
• Customized/Private Courses
• Online/self-paced curriculums
Contact: Tiffany Kelly at 412-788-1300 x217
 

 
SABRE Autonomous Solutions
 
Safety
 
Removing blasting operators from harmful environments is our key objective.
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
Fischer Technology Inc.
 
FISCHER Expands Corrosion Product Line
 
Rounding out Fischer’s extensive line of products for measuring protective coatings in the corrosion industry is the new ultrasonic wall thickness gauge UMP series.
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
Bullard
 
Upgrade with the Bullard GenVX
 
Click here for your blast helmet.
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
Vector Technologies Ltd.
 
The Original Performance Proven Vacuum Solutions
 
VecLoader® 616 Double Dump, Continuous Vacuum, 170 HP w/ 2,400 CFM & 28” Hg. 33% More Efficient than traditional vacuum systems! Choose Vector for the most powerful and the most reliable trailer mounted vacuums in the industry! Email us at: inquiry@vector-vacuums.com or call us at: 800-832-4010
 

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us