Evaluating Coatings to Control Zebra Mussel Fouling

From JPCL, November 2011

More items for Quality Control

by Allen Skaja, Ph.D.; and David Tordonato, Ph.D. U.S. Bureau of Reclamation

The authors discuss the Bureau of Reclamation’s second year of testing coatings to control zebra and quagga mussel fouling. The second year focused on non-toxic foul-release coatings. First-year results of the study have been previously published....
(Login to read the full article)


Tagged categories: Antifoulants; Shipyards

Comment Join the Conversation:

Sign in to our community to add your comments.

DeFelsko Corporation
PosiTector SST Soluble Salt Tester
Measures the concentration of soluble salts on metal surfaces. Use with all Bresle patch types including the reusable, adhesive-free PosiPatch.

Fischer Technology Inc.
Maximize Profits by Monitoring Coating Thickness
Learn more by contacting Fischer Technology today: 1.860.683.0781

Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors
Vacuum and dust collector hose, filters and related accessories.

SABRE Autonomous Solutions
Introducing the ALPHA1 Blasting Robot
Once installed and commissioned – simply

KTA-Tator, Inc. - Corporate Office
New KTA Pipeline Inspection Kit
• Defelsko standard memory body
• Positector FTS 0-250 mils, cabled dry film thickness probe
• NEW Positector Shore D hardness probe
• All essential inspection equipment!

HoldTight Solutions Inc.
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802

SAFE Systems, Inc.
Portable Blast &
Recovery Equipment
Trailer or skid mounted blast and recovery equipment. Systems designed for maximum versatility, environmental compliance
and overall cost savings.
Call 1-800-634-7278

ABKaelin, LLC
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5

Modern Safety Techniques
Modern Safety Techniques
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern

Blastox/The TDJ Group, Inc.
Blastox® - One Step Lead Abatement
Sandblast additive delivered to jobsite pre-blended to eliminate hazardous abrasive wastes. Why mix, meter or apply at the job-site? Blast with ease and
Let your painters paint!


Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL

The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us